| Recognition of Metal Fracture Surface Morphologies Based on the Fuzzy Texture Spectrum |
| ZHANG Xiaoqing; SUN Yongqing; ZHANG Zheng |
| School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083 |
|
Cite this article:
ZHANG Xiaoqing; SUN Yongqing; ZHANG Zheng. Recognition of Metal Fracture Surface Morphologies Based on the Fuzzy Texture Spectrum. Acta Metall Sin, 2004, 40(10): 1018-1022 .
|
|
|
Abstract Fuzzy uncertainty texture spectrum (FUTS) is applied for the pattern
recognition of fracture surface morphologies. Linear minor distance
classifier is used to classify five typical fracture surface
morphologies, including equiaxed dimple, elongated dimple, cleavage
failure, fatigue and intergranular cracking. With testing results,
the method of FUTS is highly efficient in fracture morphologies
classification.
|
|
Received: 31 July 2003
|
|
|
[1] Zhang D. Practical Analysis of Machinery Failure. Beijing: National Defense Press, 1997: 24(张栋.机械失效的实用分析.北京:国防工业出版社,1997:24) [2] Komai K, Minoshima K, Ishii S. JSME. Inter J (A). 1993;3(2) : 220 [3] Yan Y H, Wang D J, Huang Y H, Wang Q H, Wang T B.Acta Metall Sin, 1997; 33: 386(颜云辉,王德俊,黄雨华,王清昊,王彤波.金属学报,1997;33:386) [4] Yan Y H, Gao J H, Liu Y, Cao Y G, Lei S C. Acta Metal Sin, 2002; 38: 309(颜云辉,高金鹤,刘勇,曹宇光,雷世超.金属学报,2002;38:309) [5] Ye Y F, Zhang Z. J Mater Eng, 2003; (4) : 44(叶宇飞,张峥.材料工程,2003;(4) :44) [6] Lee Y G, Lee J H, Hsueh Y C. Neurocomputing, 1998; 20: 115 [7] Lee Y G, Lee J H, Hsueh Y C. Electron Lett, 1995; 31(12) : 959 [8] Ramze Rezaee M, Goedhart B, Lelieveldt B P E. Pattern Recognition, 1999; 32: 2011 [9] Li S Y. Fuzzy Control.Neurocontrol and Intelligent Cybernetics. Harbin: Harbin Institute of Techonology Press, 1998: 35 (李士勇.模糊控制·神经控制和智能控制论.哈尔滨:哈尔滨工业大学出版社,1998:35) [10] Bian Z Q, Zhang X G. Pattern Recognition. Beijing: Ts-inghua University Press, 1999: 186(边肇祺,张学工.模式识别.北京:清华大学出版社,1999:186) [11] American Socity For Metals ed, translated by Deng R H. Metals Handbook (8th Edition, Vol.9) . Beijing: China Machine Press, 1985: 52, 76(美国金属学会著,邓日红译.金属手册(第八版,第九卷).北京:机械工业出版社,1985:52,76) [12] Engel L, Klingele H eds, translated by Meng X M. An Atlas of Metal Damage. Beijing: China Machine Press, 1990: 32, 36, 79(Engel L,Klingele H著,孟锡明译.金属损伤图谱(下).北京:机械工业出版社,1990:32,36,79) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|