| Study Of Al--O--N And Cr--O--N Films Deposited By Arc Ion Plating As Diffusion Barriers |
| WANG Qimin; WU Yingna; JI Ailing |
| State Key Laboratory for Corrosion and Protection;Institute of Metal Research;The Chinese Academy of Sciences |
|
Cite this article:
WANG Qimin; WU Yingna; JI Ailing. Study Of Al--O--N And Cr--O--N Films Deposited By Arc Ion Plating As Diffusion Barriers. Acta Metall Sin, 2004, 40(1): 83-87 .
|
|
|
Abstract Al--O--N and Cr--O--N thin films were deposited on superalloy DSM11 by arc ion plating (AIP). The effects of flow rates of oxygen and nitrogen on phase composition and the interdiffusion of various elements at high temperature between DSM11 substrate and NiCoCrAlY coating were studied in the systems of DSM11/NiCoCrAlY, DSM11/Al--O--N/NiCoCrAlY and DSM11/Cr--O--N/NiCo- CrAlY. The results indicate that the Al(Cr)--O--N films are polycrystalline with phase constitution of α--Al2O3 + hexagonal AlN or Cr2O3+CrN , respectively. The relative intensity of AlN to
Al2O3 or CrN to Cr2O3 is changed with the change of flow rates of oxygen and nitrogen.
After oxidation at 1050℃ for 100 h, Al--O--N hindered the interdiffusion of elements between DSM11 and NiCoCrAlY more effectively than Cr--O--N film. The diffusion barrier layers hardly influenced the oxidation kinetics of the NiCoCrAlY coating.
|
|
Received: 01 January 1900
|
|
|
[1] Rhys-Jones T N. Corros Sci, 1989; 29:623 [2] Morral J E, Thompson M S. Surf Coat Technol, 1990; 43/44:371 [3] Coad J P, Rickerby D S. Mat Sci Eng, 1985; 74:93 [4] Lou H Y, Wang F H. Vacuum, 1992; 43:757 [5] Knotek O, Loffler F, Beele W. Surf Coat Technol, 1993;61:6 [6] Knotek O, Lugscheider E, L6ffier F, Beeler W. Surf Coat Technol, 1994; 68/69:26 [7] Cremer R, Witthaut M, Reichert K, Schierling M, Neuschütz D. Surf Coat Technol, 1998; 108/109:48 [8] Reichert K. Surf Eng, 1999; 15(2) : 163 [9] Müller J, Schierling M, Zimmermann E, Neuschütz D. Surf Coat Technol, 1999; 120/121:16 [10] Richthofen A V, Domnick R. Thin Solid Films, 1996; 283:37 [11] Liang Y J, Che Y C. Handbook of Thermodynamic Data for Inorganic Compounds. Shenyang: Northeast University Press, 1993: 49, 51, 122, 123(梁英教,车萌昌.无机物热力学数据手册.沈阳:东北大学出版社,1993:49,51,122,123) [12] Li M S. High Temperature Corrosion of Metals. Beijing: Metallurgy Industry Press, 2001:43(李美栓.金属的高温腐蚀.北京:冶金工业出版社,2001:43) [13] Lou H Y. J Chin Soc Corros Protect, 1997; 17(Suppl.): 464(楼翰一.中国腐蚀与防护学报.1997;17(增刊):464) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|