Comparison Of Three Turbulent Model Predictions Of Metal Flow In Aluminum Reduction Cells And Industrial Measurements
ZHOU Ping; MEI Chi; ZHOU Naijun
School of Energy and Power Engineering; Central South University
Cite this article:
ZHOU Ping; MEI Chi; ZHOU Naijun. Comparison Of Three Turbulent Model Predictions Of Metal Flow In Aluminum Reduction Cells And Industrial Measurements. Acta Metall Sin, 2004, 40(1): 77-82 .
Abstract Standard k--ε,low Reynolds' number Jones--Launder k--ε and RNG models were adopted to simulate the flow field of metal melt in three different prebaked anode cell designs, i.e.80 kA cell with three anode risers, 160 kA cell with two anode risers and 200 kA cell with four side anode risers. Moreover, the melt velocities were measured using iron rod dissolution method. The simulating results were discussed and were compared with measuring data. It is shown that the turbulent viscosity in low Reynolds' number model is smaller than that in standard k--ε model. Standard k--ε and RNG model predict better the flow field of metal melt. Furthermore, the preliminary conclusion is that the low Reynolds' number model is not suitable to calculate metal melt flow in cells if the current is greater than 80 kA.
[1] Qiu Z X. Smelting Aluminum in Prebaked Cell. Beijing: Metallurgy Industry Press, 1988:273(邱竹贤.预焙槽炼铝.北京:冶金工业出版社,1988:273) [2] Mei C. Simulation and Optimization of Non-Ferrous Metallurgical Furnaces. Beijing: Metallurgy Industry Press, 2001: 12, 152(梅炽.有色冶金炉窑仿真与优化.北京:冶金工业出版社,2001:12,152) [3] Lan X K, Khodadadi J M, Shen F. Metall Mater Trans, 1997; 28B: 321 [4] Qin K F, Fan J R. Theory and Calculation of Gas-Solid Multi-Phase Flow in Engineering. Hangzhou: Zhejiang University Press, 1989:47(岑可法,樊建人.工程气固多相流动的理论.杭州:浙江大学出版社,1989:47) [5] Ai D K. Bohner H O. Proceedings of the Technical Sessions (114th TMS Annual Meeting, Light Metals). Warrendale, Pennsylvania: Metallurgical Society of AIME, 1985:593 [6] Qiu Z X. Aluminum Electrolysis. Beijing: Metallurgy Industry Press, 1995:217(邱竹贤.铝电解.北京:冶金工业出版社,1995:217) [7] Yakhot V, Orszag S A. J Sci Computing, 1986; 1(1) : 3 [8] Li L, LI Y L. Adv Hydrodynam, 2000; 11:357(李玲,李玉梁.水力学进展,2000;11:357) [9] Zhou P, Mei C, Zhou N J. Light Met, 2002; (8) : 29(周萍,梅炽,周乃君.轻金属,2002;(8) :29) [10] Zhou P. PhD Thesis, Center South University, Changsha, 2002(周萍,中南大学博士学位论文,长沙,2002) [11] Tarapore E D. In: Peterson W S ed., Proceedings of the Technical Sessions (108th TMS Annual Meeting, Light Metals). Warrendale, Pennsylvania: Metallurgical Society of AIME, 1979:541 [12] Cai Q F, Mei C, Shen H Y. Light Metals, 1993; (9) : 29(蔡祺风,梅炽,沈洪远.轻金属,1993;(9) :29)