Mechanical Properties of Ti2SnC Particulate Reinforced Cu Matrix Composites |
YAN Chengke; ZHOU Yanchun |
Shenyang National Laboratory of Materials Science; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
YAN Chengke; ZHOU Yanchun. Mechanical Properties of Ti2SnC Particulate Reinforced Cu Matrix Composites. Acta Metall Sin, 2003, 39(1): 99-103 .
[1] Groza J R, Gibeling J C. Mater Sci Eng, 1993; A171: 115 [2] Zhou Y C, Sun Z M, Sun J H, Zhang Y, Zhou J. Z Met-allkd, 2000; 91: 329 [3] Wang X H, Zhou Y C. J Mater Chem, 2002; 12: 455 [4] Zhou Y C, Dong H Y. Mater Res Innovat, 2000; 4: 36 [5] Dong H Y, Yan C K, Chen S Q, Zhou Y C. J Mater Chem,2001; 11: 1402 [6] Zhang Y, Sun Z M, Zhou Y C. Mater Res Innovat, 1999;3: 80 [7] Zhang Y, Zhou Y C. Z Metallkd, 2000; 92: 585 [8] Petch N J. J Iron Steel Inst, 1953; 174: 25 [9] McElroy R J, Szkopiak Z C. Int Met Rev, 1972; 17: 175 [10] Zhang Y, Zhou Y C. Ada Metall Sin, 2000; 36: 662(张毅,周延春.金属学报, 2000;36:662) [11] Arsenault R J, Shi N. Mater Sci Eng, 1986; 86: 175 [12] Hansen N. Acta Metall, 1977; 25: 863+ |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|