Please wait a minute...
Acta Metall Sin  2003, Vol. 39 Issue (1): 104-108     DOI:
Research Articles Current Issue | Archive | Adv Search |
Application of the Double Shear Creep Specimens on the Fiber-Reinforced Metal Matrix Composites
YUE Zhufeng; HU Weibing; LU Zhenzhou
Department of Engineering; Mechanics; Northwestern Polytechnical University; Xi’710072
Cite this article: 

YUE Zhufeng; HU Weibing; LU Zhenzhou. Application of the Double Shear Creep Specimens on the Fiber-Reinforced Metal Matrix Composites. Acta Metall Sin, 2003, 39(1): 104-108 .

Download:  PDF(165KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  04 March 2002     
ZTFLH:  TB331  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I1/104

[1] Dong M, Schmander S. Comput Mater Sci, 1996; (5) : 53
[2] Phillips J, Staubach M, Skrotzki B, Eggeler G. Mater SciEng, 1997; A234-236: 401
[3] Cheng C, Aravas N. Int J Solid Struct, 1997; 34: 4173
[4] Nam H W, Han K S. Metall Mater Trans A, 1998; 29:1983
[5] Cseh G, Bar J, Gudladt H J, Lendvai J, Juhasz A. MaterSci Eng, 1999; A272: 145
[6] Yue Z F, Probst-Hem M, Eggeler G. Mater High Temp, 2000; 17: 449
[7] Mayr C, Eggeler G, Webster G A, Peter G. Mater Sci Eng A, 1995;199: 121
[8] Peter G, Probst-Hein M, Koolbe M, Neuking K, Eggeler G. Mater Sci Technol, 1997; 28, 457
[9] Yue Z F. Alexander von Humboldt Foundation (AvH) Report, 2000
[10] Kaustrater G, Yawny A, Schurhoff J, Skrotzki B, Eggeler G, Stockhert B. In: Parker J D ed. Creep & Fracture on Engineering Materials & Structures, Proceedings of the 9th International Conference, Swansea, 2001; April: 1
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!