Superplasticity of Large-Grained Ni-45Al |
JIANG Dongmei; LIN Dongliang |
Open Laboratory of Education Ministry of China for High Temperature Materials and Tests; School of Materials Science and Engineering; Shanghai Jiaotong University; Shanghai 200030 |
|
Cite this article:
JIANG Dongmei; LIN Dongliang. Superplasticity of Large-Grained Ni-45Al. Acta Metall Sin, 2003, 39(1): 47-50 .
[1] Lin D L, Shan A D, Li D Q. Scr Metall Mater, 1994; 31:1455 [2] Li D Q, Shan A D, Liu Y, Li D L. Scr Metall Mater, 1995;33: 681 [3] Lin D L, Shan A D, Chen M W. Intermetallics, 1996; 4:489 [4] Liu Y, Li D Q, Lin D L. Scr Metall Mater, 1996; 34: 1095 [5] Lin D L, Liu Y. Mater Sci Eng, 1999; A268: 83 [6] Gu Y F, Lin D L, Shan A D, Liu Y, Liu Z Y. Ada MetallSin, 1997; 33: 325(谷月峰,林栋梁,单爱党,刘毅,刘震云.金属学报,1997;33:325) [7] Liu Z Y, Lin D L,Gu Y F, Cao P,Lie C M, Huang B Y. Ada Metall Sin, 1996; 32: 1139(刘震云,林栋梁,谷月峰,曹鹏,雷长明,黄伯云.金属学报,1996;33:1139) [8] Sun F, Lin D L. Scr Mater, 2001; 44: 665 [9] Du X H, Guo J T, Zhou B D. Scr Mater, 2001; 45: 69 [10] Jiang D M, Lin D L. Mater Sci Lett, in press [11] Kim W Y, Hanada S, Sakai T. Mater Sci Eng, 1998; A248: 78 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|