Please wait a minute...
Acta Metall Sin  2003, Vol. 39 Issue (1): 51-54     DOI:
Research Articles Current Issue | Archive | Adv Search |
Molecular Dynamics Simulation of Tensile Stress Induced by Dealloyed Layer in Cu3Au
LI Qikai; ZHANG Yue; GUO Xianzhong; CHU Wuyang
Department of Materials Physics; University of Science and Technology Beijing; Beijing 100083
Cite this article: 

LI Qikai; ZHANG Yue; GUO Xianzhong; CHU Wuyang. Molecular Dynamics Simulation of Tensile Stress Induced by Dealloyed Layer in Cu3Au. Acta Metall Sin, 2003, 39(1): 51-54 .

Download:  PDF(143KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  19 March 2002     
ZTFLH:  TG146  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I1/51

[1] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Fracture. Beijing: Science Press, 2000: 156(褚武扬,乔利杰,陈奇志,高克玮.断裂和环境断裂.北京:科学出版社,2000:156)
[2] Jones D A. Corrosion, 1996; 52: 356
[3] Maguin T, Chieragatti R, Bayle B. Acta Mater, 1996; 44:1457
[4] Kanfman M J, Fink T L. Acta Metall, 1988; 36: 2213
[5] Gu B, Zhang J W, Wan F Y, Chu W Y. Scr Metall Mater,1995; 32: 637
[6] Gao K W, Chu W Y, Gu B, Qiao L J. Corrosion, 2000;56: 515
[7] Lu H, Gao K W, Chu W Y. Corros Sci, 1998; 40: 1663
[8] Lu H, Gao K W, Wang Y B, Chu W Y. Corrosion, 2000;56: 1112
[9] Guo X Z, Gao K W, Qiao L J, Chu W Y. Metall MaterTrans A, 2001; 32: 1309
[10] Kevin M, Ferrari M. Mater Sci Eng A, 1997; A232: 88
[11] Zhou G H, Lu H, Wan F R, Chu W Y. Ada Mech Sin,1997; 14(4) : 377
[12] Ackland G J, Vitek V. Phy Rev B, 1990-II; 41: 10324
[13] Cassagne T B, Flanagan W F, Lichter B D. Metall TransA, 1988; 19A: 281
[14] Chen T S, Salmeron M, Devine T M. Corros Sci, 1993;34: 2071
[15] Finnis M W, Sinclair J E. Philos Mag A, 1984; 50(1) : 45
[16] Toxvaerd Soren. J Comput Phys, 1982; 47: 444
[17] Vol A E, Kagan I K. Handbook of binary metallic system structure and properties, Vol.3, New Delhi: Oxonian Press PVT. Ltd., 1986: 117/
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!