Estimation of Structural Volume Fraction of Phases and Relationship Between Phase Amounts in Multi-Phase Alloys |
LIU Yan; PENG Zhifang |
College of Power and Mechanical Engineering; Wuhan University; Wuhan 430072 |
|
Cite this article:
LIU Yan; PENG Zhifang. Estimation of Structural Volume Fraction of Phases and Relationship Between Phase Amounts in Multi-Phase Alloys. Acta Metall Sin, 2003, 39(1): 22-26 .
|
|
Received: 26 February 2002
|
|
[1] Nathal M V, Ebert L J. Metall Trans, 1985; 16A: 1849 [2] Glatzel U, Feller-Kniepmeier M. Scr Metall Mater, 1991;25: 1845 [3] Melow T, Zhu J W, Wahi R P. Z Metallkd, 1994; 85: 9 [4] Lempke H, Wang Y, Mukherji D, Chen W, WiedenmannA, Wahi R P. Z Metallkd, 1994; 87: 286 [5] Schulze C, Feller-Kniepmeier M. Scr Mater, 2001; 44: 731 [6] Glatzel U. Microstructure and Internal Strains of Unde-formed and Creep Deformed Samples of a Nickel-base Su- peralloy. Berlin: Verlag Dr Koster, 1994: 10 [7] Schmidt R, Feller-Kniepmeier. Metall Trans, 1992; 23A: 745 [8] Schmidt R, Feller-Kniepmeier. Scr Metall Mater, 1992; 26: 1919 [9] Harada H, Yamazaki M, Koizumi Y, Sakuma N, Furuya N, Kamiya H. High Temperature Alloys for Gas Turbines 1982, Liege, Belgium: D.Reidel Publishing Co., 1982; 721 [10] Volkl R, Glatzel U, Feller-Kniepmeier. Scr Mater, 1998; 38: 893 [11] Peng Z F, Yan P, Luo Y S, Ren Y Y, Zhao J C. Acta Metall Sin, to be published(彭志方,燕平,骆宇时,任遥遥,赵京晨.金属学报,待发表) |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|