Solidification Behavior of a Cast Nickel-Base Superalloy
SUN Xiaofeng; YIN Fengshi; LI Jinguo; ZHENG Qi; GUAN Hengrong; HU Zhuangqi
Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 1110016; College of Mechanical Engineering; Shandong University of Technology; Zibo 255012
Cite this article: 

SUN Xiaofeng; YIN Fengshi; LI Jinguo; ZHENG Qi; GUAN Hengrong; HU Zhuangqi. Solidification Behavior of a Cast Nickel-Base Superalloy. Acta Metall Sin, 2003, 39(1): 27-29 .

Download:  PDF(137KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  11 April 2002     
ZTFLH:  TG132.3  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I1/27

[1] Yuan C, Sun X F, Yin F S, Guan H R, Hu Z Q, Zheng Q,Yu Y. J mater Sci Technol, 2001; 17: 425
[2] Yin F S Sun X F, Li Y B, Yu Y, Zhen Q, Guan H R, HuZ Q. Ada Metall Sin, 2003; 39: 75(殷凤仕,孙晓峰,李耀彪,于洋,郑启,管恒荣,胡壮麒.金属学报,2003;39:75)
[3] Li Y B, Sun X F, Zhang C Z, Yin F S, Zheng Q, Hou G C, Yu Y. Mater Mech Eng, in press(李耀彪,孙晓峰,张承忠,殷风仕,郑启,侯贵臣,于洋.机械工程材料,待发表)
[4] Burton C J. Proceedings of the Third International Symposium on Superalloys. Baton Rouge: Claitor Publishing, 1976: 147
[5] Ouichou L, Lavaud F, Lesoult G. Proceedings of the Fourth International Symposium on Superalloys. New York: American Society for Metals. 1980: 235
[6] Sponseller D L. Superalloys 1996. New York: The Minerals, Metals & Materials Society, 1996: 259
[7] Zou J, Wang H P, Doherty R, Perry E M. Superalloys 1992. New York: The Minerals, Metals & Materials Society, 1992: 165
[8] Yukawa N, Murata Y, Noda T. In: Gell M, Radvich J F eds, Superalloys 1984, Proceedings of the Fifth International Symposium on Superalloys, New York: Metallurgical Society of AIME, 1984: 83
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!