MELTING TEMPERATURES OF Fe, Co AND Ni MAGNETIC RECORDING NANOCRYSTALS
JIANG Qing; NAN Shenghui; ZHOU Ming (Department of Materials Science and Engineering; Jilin University of Technology; Changchun 130025)Correspondent: JIANG Qing; professon Tel: (431)5687607; Fax: (431)5683397;E-mail: jiangq post jut edu.cn
Cite this article: 

JIANG Qing; NAN Shenghui; ZHOU Ming (Department of Materials Science and Engineering; Jilin University of Technology; Changchun 130025)Correspondent: JIANG Qing; professon Tel: (431)5687607; Fax: (431)5683397;E-mail: jiangq post jut edu.cn. MELTING TEMPERATURES OF Fe, Co AND Ni MAGNETIC RECORDING NANOCRYSTALS. Acta Metall Sin, 1998, 34(8): 870-874.

Download:  PDF(419KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A model without any adjustable parameters, describing the dependence of melting temperature on grain size, was established. It is demonstrated that melting temperature of metallic nanocrystals decreases as its size decreases. When the size of nanocrystals reaches its minimum, the melting temperature of the nanocrystals reaches its lowest value and the corresponding melting entropy is zero. With this model, the calculated melting temperatures of in and Pb nanocrystals and Fe thin film are in correspondence with the experimental results. The melting temperatures of magnetic recording nanocrystals of Fe, Co and Ni elements are predicted.
Key words:  magnetic recording nanocrystal      radius of nanocrystal      melting entropy      melting temperature     
Received:  18 August 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I8/870

1 Saito Y, Yoshikawa T, Okuda M, Fujimoto N, Yamamuro S, Wakoh K, Sumiyama K, Suzuki K, Kasuya A,Nishina Y. Chem Phys Lett, 1993; 212: 379
2 Saito Y, Yoshikawa T, Okuda M, Fujimoto N, J Appl Phys, 1994; 75: 134
3 Klabunde K J, Zhang D, Glavee G N, Sorensen C M. Chem Mater 1994; 6: 784
4 Shi F G. J Mater Res, 1994; 9: 1307
5 Jiang Q, Aya N, Shi F G. Appl Phys, 1997; 64A: 627
6 Skripov V R, Koverda V P, SkokoV V N. Phys Status Solidi 1981; 66A: 109
7 Bourdelle K K, Johansen A, Johnson E, Sarholt-Kristensen L. Mater Sci Forum 1995; 179-181: 659
8 Thoft N B, Bohr J, Buras B, Johnson E, Jobansen A. J Phys, 1995; 28D: 539
9 Dybkjaer G, Kruse N, Johansen A, Johnson E, Sarholt-Kristensen L, Bourdelle K K. Surf Coat Technol 1996; 83: 82
10 Goldstein A N. Appl Phys, 1996; 62A: 3311 Sheng H W, ffen G, Peng L M, Hu Z Q, Lu K. PhUo8 Mag Lett, 1996; 73: 17912 Sheng H W, Ren G Peng L M, Hu Z Q, Lu K. J Mote f Rea, 1997; 12: 11913 Lai S L, Guo J Y, Petrova V, Ramanath G, Allen L H. PhW Rev Lett, 1996; 77: 9914 Childre88 J R, Chien C L, Zhou M Y, Sheng P. PhVs Rev, 1991; 44B: 11 68915 Jiang Q, Tong H Y, Hsu D T, 0kuyaIna K, Shi F G. Thin Solid Fifor 1997; 312: 35716 Jiang Q, Shi F G. i Mater Sci TeChno(1998; 14: 17117 Mitch M G, Chase S J, F0ttner J, Yu R Q, Lannin J S. PhVs Rev Lett, 1991; 67: 87518 King H W. In: Calln R W ed., Phpoicol Metalluny, New YOrk: North-Holland Publishing, 197O: 6O19 Lijima S. Nature, 1991; 354: 56
20 Ajayan P M, Lijima S. Nature, 1993; 361: 233
21 Mott N F. Proc R Soc London, 1934; 146A: 465
22 Regl A R, Glazov V M. Semiconductors, 1995; 29(5): 405
23 Lam N Q, Okamoto P R. Mater Res Bull 1994; 19(7): 41
24 Jiang Q, Zhao M, Xu X Y. Philos Mog, 1997; 76B: 1
25 Periodic Table of the Elements. Illinois: Sargent-Welch Scientific Company 1979
[1] NING Likui, ZHENG Zhi, JIN Tao, TANG Song, LIU Enze, TONG Jian, YU Yongsi, SUN Xiaofeng. EFFECT OF HEAT TREATMENTS ON THE MICROSTRUCTURE AND PROPERTY OF A NEW NICKEL BASE SINGLE CRYSTAL SUPERALLOY[J]. 金属学报, 2014, 50(8): 1011-1018.
[2] WANG Jia, XIAO Han, WU Longbiao, LU Dehong, ZHOU Rongfeng, ZHOU Rong. STUDY OF ROLLING-REMELTING SIMA PROCESS FOR PREPARING THE SEMI-SOLID BILLET OF ZCuSn10 ALLOY[J]. 金属学报, 2014, 50(5): 567-574.
No Suggested Reading articles found!