Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (7): 731-734    DOI:
Current Issue | Archive | Adv Search |
APPLICATION OF CALCIA CRUCIBLE TO MELT HIGH PURITY ALLOYS
SUN Changjie(Technical Center of Tangshan Iron & Steel Group Co. Ltd; Tangshan 063016)xING Jiping(Department of Chemical Engineering; Tangshan University; Tangshan 063001)
Cite this article: 

SUN Changjie(Technical Center of Tangshan Iron & Steel Group Co. Ltd; Tangshan 063016)xING Jiping(Department of Chemical Engineering; Tangshan University; Tangshan 063001). APPLICATION OF CALCIA CRUCIBLE TO MELT HIGH PURITY ALLOYS. Acta Metall Sin, 1998, 34(7): 731-734.

Download:  PDF(366KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new process melting the high purity alloys by using calcia crucible has been developed. The calcia crucible with excellent refining and keeping temperature properties is made successfully in 10 kg vacutun induction furnace. The purified experiment of pure iron and GH169 alloys was carried out in vacuum induction furnace and adding Al, La and Ca as cleaner. In 10 kg vacuum induction furnace and tinder condition of 1.5 - 2.5 Pa vacuum and 1400 ℃,the contents of N, O and S in alloy GH169 are reduced to less than 20×10-4%, 20×10-4% and ×10-4% from 70×10-4%, 33×10-4% and 35× 10-4%, respectively. The refilling mechanism of calcia crucible was discussed.
Key words:  vacuum induction melting      alloy purification      calcia crucible     
Received:  18 July 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I7/731

1 Woulds M J. In: Tien J K, Ototani T eds., Superalloy 1980, Proc 4th Int Symp on Superalloys, San Diego,ASM Europe, Paris, 1980: 31
2 Vaughn G A, Gerger G H. In: Bhat G K, Schlatter R eds., Proc 6th Int Conf on Vacuum Metallurgy, California,April 23 - 27, American Vacuum Society, 1979: 357
3 Brown E E, Stulga J E, Jeunings L, Sallceld R W. In: Tien J K, Ototani T eds., Superalloys 1980, Proc 4thInt Symp on Superalloys, San Diego, ASM Europe, Paris, 1980: 159
4 Holoman G P. Advanced Methods Improve Turbine Output, Precision Metal, 1980: 47
5 Tien J K, Caulfifield T. Superalloys, Supercomposites and Supereerumics. Boston: Academic, 1989: 60
6 Dailey R E, Shiring R R, Anderson R J. In: Kear B H, Muzyka D R, Tien J K, Wlodek S T eds., Superalloys:Metallurgy and manufacture. Baton Rouge: Claitor's Publ, 1976: 109
7 Fisher W A, Cohren T. Arch Eisenhuttenwes, 1950; 21: 355
8 赵炳 高铬Fe-Ni-Cr合金脱氮研究北京:冶金工业部钢铁研究总院内部资料,1982
(Zhao Bingkun. The Investigation of Denitrization Behaving to High Chromium Fe-Ni-Cr Alloy.Interna tional Material, Central Iron and Steel Research Institute, The Ministry of Metallurgical Industry Beijing,1982)
9 Ototani T, Kataura Y, Degawa T. Trans Iron Steel Inst Jpn, 1976; 16: 304
[1] JIA Lina GAO Ming GE Jingru ZHENG Lijing SHA Jiangbo ZHANG Hu. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Nb-16Si-22Ti--2Hf--2Cr--2Al INGOT PREPARED BY VACUUM INDUCTION MELTING[J]. 金属学报, 2011, 47(1): 88-94.
No Suggested Reading articles found!