| MICROSTRUCTURES AND PROPERTIES OF IN SITU SYNTHESIS Ni/Ni-Al MULTILMER COMPOSITES |
| WANG Huabin; HAN Jiecai; DU Shanyi (Center of Composite Materials; Harbin Institute of Technology; Harbin 150001) |
|
Cite this article:
WANG Huabin; HAN Jiecai; DU Shanyi (Center of Composite Materials; Harbin Institute of Technology; Harbin 150001). MICROSTRUCTURES AND PROPERTIES OF IN SITU SYNTHESIS Ni/Ni-Al MULTILMER COMPOSITES. Acta Metall Sin, 1998, 34(4): 431-436.
|
|
|
Abstract Full-dellsity Ni/Ni-Al multilayer composites were successfully fabricated by in-situ reaction of Ni and Al foils at 620℃ for 1 hour under 1 MPa pressure, and then diffusion annealing for 4 hours at 750℃, 950℃ and 1150℃ respectively under 5 MPa pressure in vacuum.Ductile Ni layer in composites can greatly improve room-temperature fracture toughness bymicrocracks bridging and blunting. After annealing at 750℃ and 950℃, Al2O3 at the surface of Al foils before reaction remains at the interface of bilayer Ni2Al3 as inclusions, which makesinterface poorly bonded. But after annealing at 1150℃, Ni3Al layer is well-bonded with Ni and NiAl layer. So, the composites show significantly strain-hardening and plastic flow, its mean fracture strength and strain are 786 MPa and 12.8% respectively.
|
|
Received: 18 April 1998
|
1Rogachev A S, Varma A, Merzhanov A G Int J SHS, 1993 2: 25 2Rogachev A S, Khomenko I O, Uarma A, Merzhanov A G Int J SHS, 1994; 3: 239 3Rawers J C; Alman D E, Hawk J A. Int J SHS, 1993; 2: 12 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|