Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (3): 225-231    DOI:
Current Issue | Archive | Adv Search |
INVESTIGATION OF THE ULTRA-FINE STRUCTURE OF SURFACE RELIEF EFFECTS ASSOCIATED WITH BAINITE IN AN Fe-C-Si-Mn ALLOY
BO Xiangzheng; FANG Hongsheng; WANG Jinjun; HUANG Weigang; ZHANG Boqing (Department of Materials Science and Engineering; Tsinghua University; Beijing 100084)
Cite this article: 

BO Xiangzheng; FANG Hongsheng; WANG Jinjun; HUANG Weigang; ZHANG Boqing (Department of Materials Science and Engineering; Tsinghua University; Beijing 100084). INVESTIGATION OF THE ULTRA-FINE STRUCTURE OF SURFACE RELIEF EFFECTS ASSOCIATED WITH BAINITE IN AN Fe-C-Si-Mn ALLOY. Acta Metall Sin, 1998, 34(3): 225-231.

Download:  PDF(2603KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Surface relief caused by the formation of lower bainite in an Fe-C-Si-Mn alloy has been investigated by STM. It was discovered that the subunit which is the lowest structural unit observed by TEM is actually made up of sub-subunits. The surface relief due to the formation of sub-subunit is tent-shaped, and of a non-IPS type, which indicates that the sub-subunit cannot be formed by shear. The height of relief is 60-140nm, and the maximum shape deformation is ca. 0.23. The multi-layer structure of bainite and the effect of carbon and silicon on the fine structure of bainite can be interpreted by sympathetic nucleation-ledgewise growth mechanism.
Key words:  STM      surface relief      sub-subunit      sympathetic nucleation-ledgewise growth     
Received:  18 March 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I3/225

1 Swallow E, Bhadeshia H K D H. Mate, Sci TechnoI, 1996; 12: 121
2 Ko T, Cottrell S A. J Iron Steel Inst, 1952; 172: 307
3 Ko T. J Iron Steel Inst, 1953; 175: 16
4 Srinivasan G R, Wayman C M. Acta Metall, 1968; 16: 609
5 Sandvik B P J. Metall Trans, l982; 13A: 789
6 Bilby B A, Christian J W. The Mechanism of Phase Transformation in Metals.London: Institute ofMetals, 1956: 121
7 Christian J W. Decooposition of Austenite by Diffusional Processes. New York: Interscience, 1962: 371
8 Clark H M, Wayman C M. Phase Transformations. Metals Park, Ohio: ASM, 1970: 59
9 Bhadeshia H K D H. Bainite in Steets. London: Institute of Materials, 1992: 51.
10 Laird C, Aaronson H I. Acta Metall, 1968; 15: 73
11 Liu Y C, Aaronson H I. Acta Metall, 1970; 18: 845
12 Hall M G, Aarouson H I. Metofl Mater Trans, 1994; 25A: 1923
13 Kinsman K R, Eichen E, Aaronson H I. Metall Trans, 1975; 6A: 303
14 Speich G R. Decomposition of Austenite by Diffusional Processes.New York:Interscience,1962: 353
15 Lee H J, Aaronson H I. Acta Metall, 1988; 36: 787
16 方鸿生, 王家军,杨志刚, 李春明, 邓旭蕊, 郑燕康. 自然科学进展, 1993; 3: 525(Fang Hongsheng, Wang Jiajun, Yang Zhigang, Li Chunming, Deng Xurui, Zheng Yankang. Prog NatSci, 1993; 3: 525)
17 Wang J J, Fang H S, Zheng Y K, Yang Z G. un Int, 1995; 35: 992
18 Binnig G, Rohrer H, Gerber Ch, Weibel E. Phys Rev Lett, 1982; 49: 57
19 Binnig G, Rohrer H. Surf Sci, 1983; 126: 236
20 俞德刚, 朱钰如, 陈大军, 唐晓宏, 张惠娟. 金属学报, 1994; 30: A385(Yu Degang, Zhu Yuru, Chen Da jun, Tang Xiaohong, Zhang Huijuan. Acta Metall Sin, 1994; 30:A385)
21 Fang H S, Wang J J, Yang Z G, Li C M, Zheng Y K, Li C X. Metall Mater bens, 1996; 27A: 1535
22 Ohmori Y. Trans Iron Steet Inst Jpn, 1971; 11: 95
23 Bhadeshia H K D H. Acta Metall, 1980; 28: 1103
24 Wechsler M S, Lieberman D S, Read T A. J Met, 1953; 197: 1503
25 Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129
26 Yang Z G, Fang H S, Wang J J, Li C M, Zheng Y K. Phys Rev, 1995; B52: 7879
27 Aaronson H I, Wells C. Trans AIME,1956; 206: 1216
28 Aaronson H I, Spanos G, Masamura R A, Vardiman T G, Moon D W, Menon E S K, Hall M G. MaterSci Eng, 1995; B32: 107
29 Reynolds W T Jr., Liu S K, Li F Z, Hartfield S, Aaronson H I. Metall Trans, 1990; 21A: 1479
30 Goldenstein H, Aaronson H I. Metall Trans, 1990; 21A: 1465
[1] SUN Baode, WANG Jun, KANG Maodong, WANG Donghong, DONG Anping, WANG Fei, GAO Haiyan, WANG Guoxiang, DU Dafan. Investment Casting Technology and Development Trend of Superalloy Ultra Limit Components[J]. 金属学报, 2022, 58(4): 412-427.
[2] WANG Xi,LIU Renci,CAO Ruxin,JIA Qing,CUI Yuyou,YANG Rui. Effect of Cooling Rate on Boride and Room Temperature Tensile Properties of β-Solidifying γ-TiAl Alloys[J]. 金属学报, 2020, 56(2): 203-211.
[3] Heng SHAO,Yan LI,Hai NAN,Qingyan XU. RESEARCH ON THE INTERFACIAL HEAT TRANSFER COEFFECIENT BETWEEN CASTING AND CERAMIC SHELL IN INVESTMENT CASTING PROCESS OF Ti6Al4V ALLOY[J]. 金属学报, 2015, 51(8): 976-984.
[4] SUN Chaoyang, SHI Bing, WU Chuanbiao, YE Naiwei, MA Tianjun, XU Wenliang, YANG Jing. HIGH TEMPERATURE CREEP DEFORMATION MECHANISM OF BSTMUF601 SUPERALLOY[J]. 金属学报, 2015, 51(3): 349-356.
[5] CHEN Yuyong, JIA Yi, XIAO Shulong, TIAN Jing, XU Lijuan. REVIEW OF THE INVESTMENT CASTING OF TiAl-BASED INTERMETALLIC ALLOYS[J]. 金属学报, 2013, 49(11): 1281-1285.
[6] SU Bin HAN Zhiqiang ZHAO Yongrang SHEN Bingzhen ZHANG Lianzhen LIU Baicheng. CA MODELING OF PHASE TRANSFORMATION IN ASTM A216 WCA CAST STEEL DURING SOLIDIFICATION AND COOLING PROCESS[J]. 金属学报, 2011, 47(11): 1388-1395.
[7] YANG Yujuan YAN Biao. THREE DIMENSIONAL MULTI-PHASE FIELD SIMULATION OF GROWTH OF EUTECTIC CBr4-C2Cl6  ALLOY
II. Effect of Lamellar Spacing on Morphology Evolution
[J]. 金属学报, 2010, 46(7): 787-793.
[8] WU Jing LIU Xinxin GU Xinfu DAI Fuzhi YANG Haitao ZHANG Wenzheng. QUANTITATIVE ANALYSIS FOR THE DISPLACEMENT OF TENT–SHAPED SURFACE RELIEF OF LATH MARTENSITE IN Fe–BASED ALLOY[J]. 金属学报, 2009, 45(12): 1425-1434.
[9] . [J]. 金属学报, 2007, 43(10): 1113-1120 .
[10] QIU Dong; ZHANG Wenzheng. MEASUREMENT AND CHARACTERIZATION OF THE SURFACE RELIEF IN A DUPLEX STAINLESS STEEL[J]. 金属学报, 2005, 41(9): 897-904 .
[11] YANG Jinbo; YANG Zhigang; BAI Bingzhe; FANG Hongsheng. Atomic Force Microscope Investigation of the Surface Relief Effect of Bainite in An Fe--C--Mn--Ni--Si Alloy[J]. 金属学报, 2004, 40(6): 574-.
[12] YIN Renhe; CAO Weimin; SHI Wenguang(Department of Chemistry; Shanghai University; Shanghai 201800)SUN Jielin(Institute of Nuclear Research; The Chinese Academy of Sciences; Shanghai 201800)MAO Bingwei; SUN Shigang(State Key Laboratory for Physics Chemistry of the Solid Surface; Xiamen University; Xiamen 361005)Correspondent: YIN Renhe; associate profsson Tel: (021)59532932-272; Fax: (021)59529932;E-mail: papayaly online. sh. ch. STUDY ON THE PROCESS OF COPPER ELECTRODEPOSITION ON PLATINUM (111)[J]. 金属学报, 1998, 34(8): 892-896.
[13] BO Xiangzheng; FANG Hongsheng( Departmetn of Materials Science and Engineering; Tsinghua University; Beijing; 100084)Correspondent: BO Xiangzheng; Tel: (010)62782361; E-mail: fhs - dms tsinghua. edu. cn.. STUDY OF THE SURFACE RELIEF EFFECTS ASSOCIATED WITH GRAIN BOUNDARY ALLOTRIOMORPHS BY SCANNING TUNNELING MICROSCOPY[J]. 金属学报, 1998, 34(8): 807-812.
[14] BO Xiangzheng; FANG Hongsheng; WANG Jiajun; WANG Zhenghua (Department of Materials Science and Engineering; Tsinghua University; Beijing 100084). STM STUDY ON THE SURFACE RELIEF EFFECTS ASSOCIATED WITH WIDMANSTATTEN FERRITE[J]. 金属学报, 1998, 34(4): 345-350.
[15] BO Xiangzheng; XU Ning; FANG Hongsheng(Department of Materials Science and Engineering; Tsinghua University; Beijing 100084)Correspondent: BO Xiangzheng; Tel: (010)62782361; Fax: (010)62771160;E-mail. As -dms @m ailTsinghua. edu. cnManuscript received 1997-12-29; in revised form 1998-03-23. STM STUDY ON THE SURFACE RELIEF EFFECTS ASSOCIATED WITH WIDMANSTAT SAWTEETH[J]. 金属学报, 1998, 34(12): 1249-1254.
No Suggested Reading articles found!