Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (2): 200-204    DOI:
Current Issue | Archive | Adv Search |
TEMPERATURE DEPENDENCE OF PERMEABILITY FOR Fe-Cu-Nb-V-Si-B NANOCRYSTALLINE ALLOY
WANG Zhi;HE Kaiyuan;YIN Jun;ZHANG Yumei;ZHANG LuO;LIANG Zhide (Department of Material Science and Engineering; Northeastern University; Shenyang 110006)(Institute of Materials Physics; Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940)
Cite this article: 

WANG Zhi;HE Kaiyuan;YIN Jun;ZHANG Yumei;ZHANG LuO;LIANG Zhide (Department of Material Science and Engineering; Northeastern University; Shenyang 110006)(Institute of Materials Physics; Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940). TEMPERATURE DEPENDENCE OF PERMEABILITY FOR Fe-Cu-Nb-V-Si-B NANOCRYSTALLINE ALLOY. Acta Metall Sin, 1998, 34(2): 200-204.

Download:  PDF(519KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The correlation between initial permeability μi and temperature T (μi-T curve) for nanocrystalline Fe72. 7 Cu 1 Nb2 V 1. 8 Si13. 5 B9 alloy annealed at 5 30 ─ 6 20℃ was investigated.The experimental results showed that the annealing temperature Ta has significant effects on μi-T curve. Three types of μi-T curves were observed. The corresponding annealing temperatures are (1) Ta=530 - 550℃t, (2) Ta=560 - 590℃ and (3) Ta 2600℃. The phase structure of alloy corresponding to the three types of μi-T curves was analysed and the effects of the grain size and volume fraction of α-Fe(Si,V) phase as well as the magnetic properties of residual amorphous phase on μi-T curve were also discussed.
Key words:  Fe-Cu-Nb-V-Si-B alloy      nanocrystalline alloy      temperature dependence of permeability     
Received:  18 February 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I2/200

1Yoshisawa Y, Ogums S, Yamauchi K.J Appl phys, 1988; 64: 6044
2Hener G. IEEE Trans Magn, 1989; MAG-25: 3327
3Hernando A, Vazquez M, Kulik T, Prados C. Phys Rev B, 1995; 51: 3581
4Varga L K, Kisdi-Koszo E, Zsoldos E, Bakos E. IEEE Trans Magn, 1994; 30: 552
5Varga L K, Bakos E, Kisdi-Koszo E, Zsoldos E, Kiss L F. J Magn Magn Mater 1994; 131: 280
6Bigot J,Lecaude N,Perron J C,Milan C,Ramiarinjaona C,Rialland J F. J Magn Magn Mater,1994;131:299
7Gawior W, Kolano R,Wojcik N.Mater,Sci Eng,1991;A133:172
8 Baricco M, Antonione C, Allia P, Tiberto P, Vinai F Mater Sci Eng, 1994; A179/A18O: 572
9 Allia P, Baricco M, Knokel M, Tiberto P, Vinai F.J Magn Magn Mater, 1994; 131: 243
10 Wang Z, He K Y, He S L, Zhang Y M, Fu Y J, Zhang L,J Magn Magn Mater,1997; 171: 300
11 Herzer G.Mater,Sci Eng,1991;A133:1
12王治,何开元,张治,金属学报,1997;33:1289 (Wang Z, He K Y, Zhang L. Acta Metall Sci, 1997; 33: 1289)
13王治,何开元,尹君,赵玉华,物理学报, 1997;46:2054(Wang Z,He K Y,Yin J, Zhao Y H. Acta Phys Sic,1997; 46:2054)
14 Wang Z, He K Y, He S L, Zhang L, Jin J, Zhang Y M, Cheng L Z. Accepted by Mater Sci Eng, 1997
[1] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
[2] Yaoxiang GENG,Xin LIN,Jianbing QIANG,Yingmin WANG,Chuang DONG. Dual-Cluster Characteristic and Composition Optimization of Finemet Soft Magnetic Nanocrystalline Alloys[J]. 金属学报, 2017, 53(7): 833-841.
[3] CHAO Yuesheng, WANG Li, ZHANG Yanhui, ZHU Hanxian, LUO Liping. EFFECT OF LOW-TEMPERATURE VACUUM ANNEALING ON THE MAGNETIC PULSED AMORPHOUS Fe52Co34Hf7B6Cu1 ALLOY[J]. 金属学报, 2012, 48(6): 749-752.
[4] LI Dingpeng SONG Xiaoyan ZHANG Zhexu LU Nianduan QIAO Yinkai LIU Xuemei. PREPARATION AND PROPERTIES OF SINGLE–PHASE Sm5Co2 NANOCRYSTALLINE ALLOY[J]. 金属学报, 2012, 48(10): 1248-1252.
[5] LIANG Haining SONG Xiaoyan ZHANG Zhexu LU Nianduan LIU Xuemei ZHANG Jiuxing. PREPARATION AND CHARACTERIZATION OF SmCo2 NANOCRYSTALLINE ALLOY WITH PERMANENT MAGNETIC PROPERTIES[J]. 金属学报, 2010, 46(8): 973-978.
[6] WANG Zhi;HE Kaiyuan;ZHANG Luo (Northeastern University; Shenyang 110006)(Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940). MAGNETOTHERMAL ANALYSIS OF Fe_(72.7)Cu_1Nb_2V_(1.8)Si_(13.5)B_9 ALLOY[J]. 金属学报, 1997, 33(12): 1289-1294.
[7] PING Dehai;QIN Hiaoying;LI Douxing;ZHANG Lide;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Institute of Solid State Physics;Chinese Academy of Sciences;Hefei 230031)(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-12-25). A MICROSTRUCTURAL EVOLUTION OF Ag-Cu NANOCRYSTALLINE ALLOYS[J]. 金属学报, 1996, 32(10): 1087-1092.
[8] PING Dehai; (Laborutory of Atornic Imaging of Solids; Inslitute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) XIE Miansheng; JIN Zhixiong; LI Douxing; YE HenKqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Cthinese Academy of Sciences; Shenyang 110015). PREPARATION AND PROPERTIES OF NANOCRYSTALLINE Ti_(70)Ni_(20)Si_(10) ALLOY[J]. 金属学报, 1995, 31(17): 200-205.
[9] ZHANG Yanzhong; (Shanghai Iron and Steel Research Institute; ShanHhai 200940) NIAN Suzhen; JIN Huijuan; XU Guiqin (Shanghai Iron and STeel Research Instituie; Shanghai 200940 ); YANG XielonK; LI Xiangqing(East China Normal University; Shanghai 200062). MAGNETIC PROPERTIES OF NANOCRYSTALLINE Fe_(74.7-X)Cu_1Nb_xV_(1.8)Si_(13.5)B_9 ALLOYS[J]. 金属学报, 1995, 31(17): 212-219.
[10] LU Zhichao; XIANYU Ze (Department of Physics; Northeastern University;Shenyang)SHEN Baogen((Institute of Physics; Chinese Academy of Scicnces;Beijing)LU Manqi(Institute of Metal Research; Chinese Academy of Sciences;Shenyang). THERMAL EXPANSION AND MAGNETIC PROPERTIES OF NANOCRYSTALLINE Fe-Zr-B ALLOYS[J]. 金属学报, 1994, 30(18): 265-269.
[11] BAI Kuichang;JIANG Ziying;HE Kaiyuan;CHENG Lizhi;ZHI Jing(Northeastern University;Shenyang)(Manuscript received 7 June;1993;in revised form 9 August;1993). STRUCTURAL STUDY OF NANOCRYSTALLINE Fe-Cu-Nb-Si-B ALLOYS BY MSSBAUER SPECTROSCOPY[J]. 金属学报, 1994, 30(14): 66-71.
[12] ZHI Jing;HE Kaiyuan;CHENG Lizhi;FU Yujun;WANG Zhi;LIU Yi (Northeastern University;Shengyang)(Manuscript received 30 January 1993:in revised form 25 June;1993). MICROSTRUCTURE AND MAGNETIC PROPERTIES OF NANOCRYSTALLINE(Fe,Cu,Nb)_(77.5)Si_xB_(22.5-x) ALLOYS[J]. 金属学报, 1994, 30(14): 61-65.
[13] LIU Xuedong;ZHU Jie;JIANG Jian;DING Bingzhe;WANG Jingtang Institute of Metal Research. Academia Sinica; Shenyang. STRUCTURE OF NANOCRYSTALLINE Fe-Cu-Si-B ALLOYS[J]. 金属学报, 1993, 29(9): 72-76.
[14] ZHANG Yanzhong Shanghai Iron and Steel Research Institute; Shanghai. MAGNETIC PROPERTIES OF NEW NANOCRYSTALLINEFe_(71.5)(CuCrV)_(7.5)Si_(12)B_9 SOFT MAGNETIC ALLOY[J]. 金属学报, 1993, 29(10): 82-86.
[15] TONG Huayu;DING Bingzhe;JIANG Honggang;LI Shuling;LI Gusong;WANG Jingtang State Key Laboratory of RSA; Institute of Metal Research; Academia Sinica; Shenyang Correspondent Research assistant; Institute of Metal Research; Academia Sinica; Shenyang 110015. THERMAL PROPERTIES OF NANOCRYSTALLINE Fe_(78)B_(13)Si_9 ALLOY[J]. 金属学报, 1992, 28(6): 71-75.
No Suggested Reading articles found!