Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (12): 1243-1248    DOI:
Current Issue | Archive | Adv Search |
RELATIONSHIP BETWEEN PARTIAL AND AVERAGE ATOMIC VOLUMES OF COMPONENTS IN Cu-Ni ALLOYS
XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; ChangSha 410083)CorrsPondent: XIE Youqing; pwtsson Tel: (O731)8879287; Fax: (0731)8826136Manuscript received 1997-12-1; in revised form 1998-0406
Cite this article: 

XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; ChangSha 410083)CorrsPondent: XIE Youqing; pwtsson Tel: (O731)8879287; Fax: (0731)8826136Manuscript received 1997-12-1; in revised form 1998-0406. RELATIONSHIP BETWEEN PARTIAL AND AVERAGE ATOMIC VOLUMES OF COMPONENTS IN Cu-Ni ALLOYS. Acta Metall Sin, 1998, 34(12): 1243-1248.

Download:  PDF(502KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  General equations of relationship between partial and average molar propertiesof alloy components and functions of partial molar properties in CC theory have been established.The differential equation and its constraining equation between partial and average molar proWerties and general Gibbs--Duhem formula have been derived. It has been proved that the partialmolar properties calculated from various combinative functions of average molar properties areequal, but in general the partial molar properties are not equal to the average molar propertiesof a given component. All equations and functions established in this paper have been provedto be correct by calculations of partial and average atomic volumes of components and averageatomic volumes of the solid solutions in the Cu-Ni system.
Key words:  Cu-Ni alloy      average molar property      partial molar property      atodric volume      lattice constant     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I12/1243

1谢佑卿.中国科学,1997;E27:488(Xie Y Q.SCi Chin,1998; E41:146)
2谢佑卿,张晓东中国科学,1998;E28:12(Xie Y Q, Zhang X D. Sci Chin, 1998; E41: 157)
3 Walter J M. Physical Chemistry London: Longman Group Limited; 1976: 230
4谢佑卿,张晓东金属学报,1994;A30:531(Xie Y Q, Zhang X D. Acta Metall Sin, 1994; A30: 531)
5谢信卿,马柳莺,张晓东等.中国科学,19932 A23:999(Xie Y Q, Ma L Y, Zhang X D et al. Sci Chin, 1993; A36: 612)
[1] LIU Yongkang, HUANG Haiyou, XIE Jianxin. ANISOTROPIC DEFORMATION BEHAVIOR OF CONTINUOUS COLUMNAR-GRAINED CuNi10Fe1Mn ALLOY[J]. 金属学报, 2015, 51(1): 40-48.
[2] WANG Yanqiu, SHAO Yawei, MENG Guozhe, ZHANG Tao,WANG Fuhui. STUDY ON PASSIVATING TREATMENT OF Cu-Ni ALLOY IN COMPOUND PASSIVANT CONTAINING BENZOTRIAZOLE[J]. 金属学报, 2012, 48(6): 744-748.
[3] XU Qunjie DENG Xianqin PAN Hongtao YUN Hong. ELECTROCHEMICAL BEHAVIOR OF B30 Cu-Ni ALLOY WITH SUPER-HYDROPHOBIC SURFACE IN 3.5%NaCl SOLUTION[J]. 金属学报, 2012, 48(1): 94-98.
[4] WANG Youdao WU Erdong WANG Sucheng LI Wuhui. X-RAY DIFFRACTION ANALYSIS ON THE THICKNESS EFFECT OF γ/γ' LATTICE MISMATCHE IN NICKEL BASE SINGLE CRYSTAL SUPERALLOY DD10[J]. 金属学报, 2011, 47(11): 1418-1425.
[5] ZHANG Jie WANG Qing WANG Yingmin DONG Chuang. STUDY ON THE CLUSTER--BASED MODEL OF Ni30Cu70 SOLID SOLUTION WITH Fe AND Mn AND ITS CORROSION RESISTANCE[J]. 金属学报, 2009, 45(11): 1390-1395.
[6] ;. Inhibition Action and Mechanism of the Self-assembled Monolayers of 3-amino-1,2,4-triazole on Cu-Ni Alloy[J]. 金属学报, 2008, 44(2): 203-208 .
[7] XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; Changsha 410083)Correspondent:XIE Youqing; professor; Tel: (0731)8879287; Fax. (O731)8826136Manuscript received 1997-11-14; in revised form 1998-02-12. LATTICE CONSTANTS OF DISORDERED AND ORDERED PHASES IN Au-Cu SYSTEM[J]. 金属学报, 1998, 34(12): 1233-1242.
[8] XIE Youqing;ZHANG Hiaodong(Central South University of Technology; Changsha). MICROSTRUCTURE AND PROPERTIES OF Au-Cu ALLOYS[J]. 金属学报, 1994, 30(12): 531-539.
[9] XU Wenchong;SUN Fuyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing XU Wenchong; senior engineer; Department Institute; Ministry of Metallurgical Industry No;13. Central Iron and SteelResearch Beijing 100081. LATTICE PARAMETERS OF COMPLEX CARBONITRIDE CONTAINING Ti, Nb AND V[J]. 金属学报, 1989, 25(6): 146-148.