Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (11): 1126-1130    DOI:
论文 Current Issue | Archive | Adv Search |
ELECTRICAL PROPERTIES OF Fe_3Al INTERMETALLICS
YU Xinquan;SUN Yangshan;MEI Jianping;SUN Guoxiong (Department of Materials Science and Engineering;Southeast University; Nanjing 210096)
Cite this article: 

YU Xinquan;SUN Yangshan;MEI Jianping;SUN Guoxiong (Department of Materials Science and Engineering;Southeast University; Nanjing 210096). ELECTRICAL PROPERTIES OF Fe_3Al INTERMETALLICS. Acta Metall Sin, 1998, 34(11): 1126-1130.

Download:  PDF(441KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The electrical properties of Fe3Al intermetallics have been studied. The results indicate that the binary Fe3Al alloys have high electrical resistivity which relates to Al content. Additions of alloying elements further increase the electrical resistivity. An anomalous relationship between resistivity and temperature has been found in the temperature range of 20-1100℃,and the mechanism of the phomenon has also been discussed.

Key words:  Fe_3Al      electrical properties      electrical resistivity      Fe_3Al      electrical properties      electrical resistivity     
Received:  18 November 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I11/1126

1Mckamey C G, Devan J H, Tortoreli P T; Sikka V K. J Mater Res, 1991; 6: 1779
2何开元精密合金材料北京:冶金工业出版社,1991:226(He K Y. Precison Alloy Material.Beijing:Metallurgical Insdustry Press,1991:226)
3顾秉林,王喜坤.固体物理.北京:清华大学出版社。1989:209(Gu B L,Wang X K.Solid State Phys.Beijing:Qinghua Universsity Press,1989:209)
4 Dugdale J S. The Electrical Properties of Metals and Alloys. Edward Arhold(publishers) Ltd, 1977: 114
5 Hyde T A, Sellers C H, Wright J K, Wright R N.Scr Metall, 1993;1: 113
6 Lawlsy A; Vidoz E A、 Cahn R W Acta Metall, 1961; 9: 287
7 Anderson P W.Phys Rev,1958;109:1492
[1] ZENG Xiaoqin, WANG Jie, YING Tao, DING Wenjiang. Recent Progress on Thermal Conductivity of Magnesium and Its Alloys[J]. 金属学报, 2022, 58(4): 400-411.
[2] SUN Xiaojun, HE Jie, CHEN Bin, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HAO Hongri. Effect of Fe Content on the Microstructure, Electrical Resistivity, and Nanoindentation Behavior of Zr60Cu40-xFex Phase-Separated Metallic Glasses[J]. 金属学报, 2021, 57(5): 675-683.
[3] Rui YANG,Yan PAN,Wei CHEN,Qiaoyan SUN,Lin XIAO,Jun SUN. DEFORMATION BEHAVIOR AND THE MECHANISM OF MICRO-SCALE Ti-10V-2Fe-3Al PILLARSIN COMPRESSION[J]. 金属学报, 2016, 52(2): 135-142.
[4] Xiaowei ZUO,Rui GUO,Bailing AN,Lin ZHANG,Engang WANG. MICROSTRUCTURE, HARDNESS AND ELECTRICAL RESISTIVITY OF DIRECTIONALLY SOLIDIFIEDCu-6%Ag ALLOY UNDER A TRANSVERSE MAGNETIC FIELD[J]. 金属学报, 2016, 52(2): 143-150.
[5] HongMing Zhou. PREPARATION OF ALUMINIUM DOPED ZINC OXIDE FILMS AND THE STUDY OF THEIR MICROSTRUCTURE, ELECTRICAL AND OPTICAL PROPERTIES[J]. 金属学报, 2006, 42(5): 505-510 .
[6] ZHENG Weiwei;YANG Wangyue;LIU Qing;SUN Zuqing(Department of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083). ROOM TEMPERATURE MECHANICAL BEHAVIOR OF B2-ORDERED Fe_3Al SINGLE CRYSTALS[J]. 金属学报, 1998, 34(11): 1137-1142.
[7] SUN Yangshan;YU Xinquan;HUANG Haibo;SUN Guoxiong (Department of Materials Science and Engineering; Southeast University; Nanjing 210096). OXIDATION RESISTANCE OF Fe_3Al INTERMETALLICS AT HIGH TEMPERATURES[J]. 金属学报, 1998, 34(11): 1131-1136.
[8] ZHANG Zhonghua; SUN Yangshan; LIU Guijun (Southeast University; Nanjing 210096). IMPROVEMENT OF ROOM TEMPERATURE ENVIRONMENTAL BRITTLEMENT OF Fe_3Al-BASED ALLOY BY ELECTRO-BRUSH PLATING[J]. 金属学报, 1996, 32(9): 955-958.
[9] YANG Wangyue; SHENG Lizhen;SUN Zuqing; HUANG Yuanding; MAO Weimin (University of Science and Technology Beijing; Beijing 100083); ZHANG Baisheng; YE Chuntang (China Institute of Atomic Energy; Beijing 102413)(Manuscript received 1995-11-10; in revised form 1996-04-05). NEUTRON DIFFRACTION STUDY ON SITE OCCUPATION OF SUBSTITUTIONAL ELEMENTS AT SUBLATTICE IN Fe_3Al INTERMETALLICS[J]. 金属学报, 1996, 32(8): 799-804.
[10] WENG Jun; ZHU Fengwu; ZHI Rentao; WANG Shuangquan; XIAO jimei (University of Scicnce and Technology Beijing; Beijing 100083)(Manuscript received 1995-12-18). FIM OBSERVATION ON B2 ORDERING IN Fe_3Al ALLOY[J]. 金属学报, 1996, 32(7): 695-699.
[11] ZHAO Zhongtao; LIU Tao; MA Ruzhang (University of Scicnce and Technology Beijing; Beijing 100083); MA Changying (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081 ). ON THE PRECIPITATE IN Fe-28Al ALLOY[J]. 金属学报, 1996, 32(6): 585-588.
[12] ZHANG Jianmin(Central Iron and Steel Research Institute;Ministry;of Metallurgical Industry;Beijing 100081)ZHANG Ruilin;YU Ruihuang(Jilin University;Changchun 130023)(Manuscript received 1994-08-29;in revised form 1995-02-05). HYDROGEN EMBRITTLEMENT BEHAVIOUR IN Fe_3Al[J]. 金属学报, 1995, 31(7): 300-303.
[13] CHEN Mingwei; SHAN Aidang; LIN Dongliang(Shanghai Jaiotong University Shanghai 200030); LIANG Wei(Taiyuan University of Technology; Taiyuan 030024). IN SITU RECRYSTALLIZATION DURING ELEVATED TEMPERATURE DEFORMATION IN Fe_3Al BASED ALLOY[J]. 金属学报, 1995, 31(4): 165-169.
[14] SHAN Aidang;LIN Dongliang; CHEN Mingwei; LI Dingqiang(Shanghai Jiaotong Universitty; Shanghai 200030)(Manuscript received. 94-05-12). SUPERPLASTICITY IN Fe_3Al ALLOY WITH LARGE GRAINS[J]. 金属学报, 1995, 31(13): 35-39.
[15] GAO Hiaomei; QIAN Xiangrong (Shanghai Iron and Steel Research Institute)(Manuscript received 3 May; 1993; in revised form 20 January; 1994). XPS STUDY ON TOUGHENING EFFECT OF Cr IN Fe_3Al[J]. 金属学报, 1994, 30(7): 307-311.
No Suggested Reading articles found!