Acta Metall Sin  1997, Vol. 33 Issue (2): 222-224    DOI:
Current Issue | Archive | Adv Search |
RARE METALS IN CHINA
L.Zhou and W.H. Yin (Northwest Institute for Nonferrous Metal Research; Xi'an 710016)
Cite this article: 

L.Zhou and W.H. Yin (Northwest Institute for Nonferrous Metal Research; Xi'an 710016). RARE METALS IN CHINA. Acta Metall Sin, 1997, 33(2): 222-224.

Download:  PDF(266KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A brief account of the development of rare metals research and production in China.
Key words:  rare metals      China     
Received:  18 February 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I2/222

[1] XUE Kemin, SHENG Jie, YAN Siliang, TIAN Wenchun, LI Ping. Influence of Precipitation of China Low Activation Martensitic Steel on Its Mechanical Properties After Groove Pressing[J]. 金属学报, 2021, 57(7): 903-912.
[2] Anhua LI, Yueming ZHANG, Haibo FENG, Ning ZOU, Zhongshan Lü, Xujie ZOU, Wei LI. Mechanical Properties of Sintered Ce-Fe-B Magnets[J]. 金属学报, 2017, 53(11): 1478-1486.
[3] XUE Yingyu, TANG Jiancheng, ZHUO Haiou, YE Nan, WU Tong, ZHOU Xusheng. MICROSTRUCTURES AND PROPERTIES OF LEAD-FREE FREE-CUTTING GRAPHITE-BRASS PREPARED BY GRAPHITIZATION OF CEMENTITE[J]. 金属学报, 2015, 51(2): 223-229.
[4] ZHANG Shourong (Wuhan Iron and Steel Corporation; Wuhan 430083). EVALUATION OF TECHNOLOGICAL POLICY OF IRONMAKING IN CHINA[J]. 金属学报, 1997, 33(1): 22-28.
No Suggested Reading articles found!