SAFETY ANALYSIS OF RIVETED BRIDGES BASED ON FRACTURE MECHANICS
W. Dahl and P. Langenberg(Institute of Ferrous Metallurgy; RWTH Aachen; Germany)
Cite this article: 

W. Dahl and P. Langenberg(Institute of Ferrous Metallurgy; RWTH Aachen; Germany). SAFETY ANALYSIS OF RIVETED BRIDGES BASED ON FRACTURE MECHANICS. Acta Metall Sin, 1997, 33(2): 175-186.

Download:  PDF(874KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A simplified method of safety analysis of riveted bridges based on fracture mechanics is presented in this paper First a new formula for the calculation of the fracture load of a brjdge member with an assumed crack. has been derived from new FEM-calculations.Second. a population of more than 400 experimental strength and fracture mechanic values derived from material taken from riveted bridges build between 1890 and 1930has been evaluated statistically to derive characteristic distributions as a basis for the material input data of the fracture mechanic concept. Third, large scale tests with oldbridge plates using the plane plate geometries described above bearing artificially pro-duced cracks have been carried out to verify the proposed method by comparing pre-dicted with experimental results. Fourth the new formula has been applied for modern structural steels with yield strength from 350 t0 890 MPa and large scale tests per-formed on the large sale testing machine at the Institute of Ferrous Metallurgy in sever-al research projects have re-evaluated to find out the quality of this approach.
Key words:  fracture mechanics      finite element simulation      safety of riveted bridge     
Received:  18 February 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I2/175

1 W.Dahl, O.Schumann and G. Sedlacek, IABSE Workshop Remaining Fatigue Life Of Steel Structures Lausanne 1990, IABSE Report 59 (1990)31 3.
2 W.Hensen, Dissertation RWTH Aachen, 1992, Schriftenreihe Stahlbau RWTH Aachen, Heft 21.
3 J. Milne, R.A. Ainsworth, A.R. Dowling and A.T. Stewart. ICEGB-R/H/ R6 Rev.J, UK, 1986.
4 C.Beltrami, DLcsertation RWTH Achen, 1995, Berichte aus dem Institite fur Eisenhuttenkunde, Band 5,1995.
5 T.T.Shih, Eng. Fract. Mech. 13 (1980) 257.
6 K. Wallin, Statistic modelling in the ductile-to-brittle transitionregion, in Defectassesment in Components-Fundamentals and Aplications, LSIS. EGF9, eds. J. Blauel and K.H. Schwalbe(Mechenical Engineering Publications, London, 1991 ) 415.
7 J. Heerens, U. Zerbst and K. H. Schwalbe- Fatigue Fract. Eng. Mater. Struct. 16 (1993) 1213.
[1] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[2] CHEN Yongjun, BAI Yan, DONG Chuang, XIE Zhiwen, YAN Feng, WU Di. Passivation Behavior on the Surface of Stainless Steel Reinforced by Quasicrystal-Abrasive via Finite Element Simulation[J]. 金属学报, 2020, 56(6): 909-918.
[3] WANG Xia, WANG Wei, YANG Guang, WANG Chao, REN Yuhang. Dimensional Effect on Thermo-Mechanical Evolution of Laser Depositing Thin-Walled Structure[J]. 金属学报, 2020, 56(5): 745-752.
[4] JIANG Lin, ZHANG Liang, LIU Zhiquan. Effects of Al Interlayer and Ni(V) Transition Layer on the Welding Residual Stress of Co/Al/Cu Sandwich Target Assembly[J]. 金属学报, 2020, 56(10): 1433-1440.
[5] MA Kai, ZHANG Xingxing, WANG Dong, WANG Quanzhao, LIU Zhenyu, XIAO Bolv, MA Zongyi. Optimization and Simulation of Deformation Parameters of SiC/2009Al Composites[J]. 金属学报, 2019, 55(10): 1329-1337.
[6] Shu WEN, Anping DONG, Yanling LU, Guoliang ZHU, Da SHU, Baode SUN. Finite Element Simulation of the Temperature Field and Residual Stress in GH536 Superalloy Treated by Selective Laser Melting[J]. 金属学报, 2018, 54(3): 393-403.
[7] Jialin LIU, Yumin WANG, Guoxing ZHANG, Xu ZHANG, Lina YANG, Qing YANG, Rui YANG. Research on Single SiC Fiber Reinforced TC17 CompositesUnder Transverse Tension[J]. 金属学报, 2018, 54(12): 1809-1817.
[8] Yu LIU, Shengwei QIN, Xunwei ZUO, Nailu CHEN, Yonghua RONG. Finite Element Simulation and Experimental Verification of Quenching Stress in Fully Through-Hardened Cylinders[J]. 金属学报, 2017, 53(6): 733-742.
[9] FENG Rui, ZHANG Meihan, CHEN Nailu, ZUO Xunwei, RONG Yonghua. FINITE ELEMENT SIMULATION OF THE EFFECT OF STRESS RELAXATION ON STRAIN-INDUCED MARTENSITIC TRANSFORMATION[J]. 金属学报, 2014, 50(4): 498-506.
[10] LIU Renci, WANG Zhen, LIU Dong, BAI Chunguang, CUI Yuyou, YANG Rui. MICROSTRUCTURE AND TENSILE PROPERTIES OF Ti-45.5Al-2Cr-2Nb-0.15B ALLOY PROCESSED BY HOT EXTRUSION[J]. 金属学报, 2013, 49(6): 641-648.
[11] XU Jiayu CHEN Hongtao LI Mingyu. STUDY ON LEAD-FREE SOLDER JOINT RELIABILITY BASED ON GRAIN ORIENTATION[J]. 金属学报, 2012, 48(9): 1042-1048.
[12] WU Bo WEI Yueguang TAN Jiansong WANG Jianping. NUMERICAL SIMULATIONS OF THE INTERGRANULAR FRACTURE IN NANOCRYSTALLINE Ni[J]. 金属学报, 2009, 45(9): 1077-1082.
[13] SHI Yanke ZHANG Keshi HU Guijuan. SUBSEQUENT YIELD AND PLASTIC FLOW ANALYSIS OF POLYCRYSTALLINE COPPER UNDER BIAXIAL LOADING[J]. 金属学报, 2009, 45(11): 1370-1377.
[14] Guo-Dong ZHANG. Finite Element Simulation for Welding Residual Stress and Creep Damage of Welded Joint[J]. 金属学报, 2008, 44(7): 848-852 .
[15] . [J]. 金属学报, 2006, 42(5): 454-458 .
No Suggested Reading articles found!