Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (9): 993-997    DOI:
Current Issue | Archive | Adv Search |
DIRECTIONAL GROWTH OF EUTECTIC Al-Li COMPOSITE MATERIALS
PENG Delin; MIN Guanghui; AN Geying; LIU Hongbo (Harbin Institute of Technology; Harbin 150001)
Cite this article: 

PENG Delin; MIN Guanghui; AN Geying; LIU Hongbo (Harbin Institute of Technology; Harbin 150001). DIRECTIONAL GROWTH OF EUTECTIC Al-Li COMPOSITE MATERIALS. Acta Metall Sin, 1996, 32(9): 993-997.

Download:  PDF(415KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The crystal growth criterion was studied to obtain eutectic composite materials for hypoeutectic Al-Li alloy. It is shown that the solid/liquid interface exhibits a stable and planar form and the ragular eutectic structure can be obtained when 6.5×10~5 K·s·cm~(-2)≤ G_L/R< 11×10~5K·s·cm~(-2). The morphology of β phase (AlLi) is bar-like in Al-Li eutectic structure.
Key words:  Al-Li alloy      eutectic composite material      directional solidification     
Received:  18 September 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I9/993

1HagneslllTG,WyteM.Proceedingsof4thInternationalAl-LiConference,Paris,LesEditionsdePhysique,1987:6022WebsterD,HayneslllTG,FlemingRG.MetProg,1988;6:253SpilkerJ,NolteM,Schadlich-StubenrauchJ,SahmPR.Proceedingsof6thInternationalAl-LialloyConference,Garmisch-Partenkirchen,1991:8954ChenSW,JanCH,LinJC,ChangYA.MetallTrans,1989;20A:22475MinaminoY,YamaneT,ArakiH.MetallTrans.1987;18A:15366SchaeterRJ,CoriellSR.MetallTrans,1984;15A:21097McFadderGB,CorielSR,BoisvertRF,GlicksmanME,FangQT.MetallTrans,1984;15A:21178McFadderGB,RehmRG,CoriellSR,ChuekW,MorrishKA.MetallTrans,1984;15A:21259CoriellSR,McFaddenB,BoisvertRF,JCrystGrowth,1984;66:514
[1] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[2] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[3] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[4] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[5] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
[6] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[7] ZHANG Xiaoli, FENG Li, YANG Yanhong, ZHOU Yizhou, LIU Guiqun. Influence of Secondary Orientation on Competitive Grain Growth of Nickel-Based Superalloys[J]. 金属学报, 2020, 56(7): 969-978.
[8] LI Shiju, LI Yang, CHEN Jianqiang, LI Zhonghao, XU Guangming, LI Yong, WANG Zhaodong, WANG Guodong. Segregation Behavior, Microstructure and Properties of 2099Al-Li Alloy Produced by Twin-Roll Casting Underthe Action of Electromagnetic Oscillation Field[J]. 金属学报, 2020, 56(6): 831-839.
[9] XU Qingyan,YANG Cong,YAN Xuewei,LIU Baicheng. Development of Numerical Simulation in Nickel-Based Superalloy Turbine Blade Directional Solidification[J]. 金属学报, 2019, 55(9): 1175-1184.
[10] ZHANG Jian,WANG Li,WANG Dong,XIE Guang,LU Yuzhang,SHEN Jian,LOU Langhong. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2019, 55(9): 1077-1094.
[11] Chao CAI,Yang LI,Jinfeng LI,Zhao ZHANG,Jianqing ZHANG. Correlation Between Ageing Precipitation, Potential and Intergranular Corrosion of 2A97 Al-Li Alloy Sheet[J]. 金属学报, 2019, 55(8): 958-966.
[12] Xu LI,Qingbo YANG,Xiangze FAN,Yonglin GUO,Lin LIN,Zhiqing ZHANG. Influence of Deformation Parameters on Dynamic Recrystallization of 2195 Al-Li Alloy[J]. 金属学报, 2019, 55(6): 709-719.
[13] Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU. Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:[J]. 金属学报, 2019, 55(5): 664-672.
[14] Yan YANG, Guangyu YANG, Shifeng LUO, Lei XIAO, Wanqi JIE. Microstructures and Growth Orientation of Directionally Solidification Mg-14.61Gd Alloy[J]. 金属学报, 2019, 55(2): 202-212.
[15] JIN Hao, JIA Qing, LIU Ronghua, XIAN Quangang, CUI Yuyou, XU Dongsheng, YANG Rui. Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy[J]. 金属学报, 2019, 55(12): 1519-1526.
No Suggested Reading articles found!