CORROSION OF Fe-Cr-Mn ALLOY CONTAINING EUTECTIC CARBIDE UNDER SULFUR ATMOSPHERE
XING Jiandong; WANG Wenhu; GAO Yimin; WANG Enzhe(Xi'an jiaotong University; Xi'an 710049)(Manuscript received 1995-04-17; in revised form 1995-11-13)
Cite this article: 

XING Jiandong; WANG Wenhu; GAO Yimin; WANG Enzhe(Xi'an jiaotong University; Xi'an 710049)(Manuscript received 1995-04-17; in revised form 1995-11-13). CORROSION OF Fe-Cr-Mn ALLOY CONTAINING EUTECTIC CARBIDE UNDER SULFUR ATMOSPHERE. Acta Metall Sin, 1996, 32(2): 191-196.

Download:  PDF(523KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Corrosion test at 800℃ was carried out in mixed sulfur atmosphere for Fe-Cr-Mn alloys containing various contents of C ranging from 0.50 % to 2.63 %. The types and relative contents of corrosion scale were analyzed by X-ray diffraction. The distribution of elements and corrosion behaviour of eutectic carbide were examined. Results show that the corrosion resistance of the studied alloys is better than that of high Ni heat resisteant steel. The corrosion behaviour of alloys under tested conditions is controlled by the sulphuration and oxidation corrosion and so make a peak value of the mass gain of the alloys.With the strengthening of oxidational atmosphere the peak value is moved toward low carbon side. The eutectic carbide is more corrosion resistant than matrix.(Correspondent: XING Jiandong, professor, College of Mechanical Engineering, Xi'an Jiaotong University,Xi'an 710049)
Key words:  sulfur corrosion      eutectic carbide      heat resistant alloy     
Received:  18 February 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I2/191

1 XingJiandong,LuWenhua,WangXiaotong.In:LudemaKCed.,WearofMaterials,IntConfonwearofMaterials,NewYork:ASME,1983:452YanPing,ZhouQingde.In:LudemaKCed.,WearofMaterials,IntConfonWearofMaterials,Houston:ASME,1987:7423SuJunyi,JiaYuding.In:LudemaKCed.,WearofMaterials,IntConfonWearofMaterials,Houston:ASME,1987:6664邢建东,周庆德.摩擦磨损,1989(1):285赵学增,邢建东,周庆德.金属学报,1992;28:B2536张安峰,邢建东,陆文华.金属学报,1993;29:B263
[1] ZHANG Shihong, HU Kai, LIU Xia, YANG Yang. Corrosion-Erosion Mechanism and Research Prospect of Bare Materials and Protective Coatings for Power Generation Boiler[J]. 金属学报, 2022, 58(3): 272-294.
[2] ZHOU Xuefeng, FANG Feng, TU Yiyou, JIANG Jianqing, XU Huixia, ZHU Wanglong. EFFECT OF ALUMINUM ON THE SOLIDIFICATION MICROSTRUCTURE OF M2 HIGH SPEED STEEL[J]. 金属学报, 2014, 50(7): 769-776.
[3] LUAN Yikun BAI Yunlong SONG Nannan KANG Xiuhong LI Dianzhong. HEAT TREATMENT OF HIGH SPEED STEEL USED FOR CENTRIFUGAL CAST ROLLS[J]. 金属学报, 2009, 45(4): 470-475.
[4] LI Yanjun; JIANG Qichuan; ZHAO Yuguang; HE Zhenming(Jilin University of Technology; Changchun 130025) (Manuscript received 1 995-10-06). MODIFICATION OF M2 CAST HIGH SPEED STEEL[J]. 金属学报, 1996, 32(3): 313-317.
[5] WANG Shuqi;JIANG Qichuan;ZHAO Yuguang;HE Zhenming(Jilin University of Technology;Changchun 130025)(Manuscript received 1994-11-11;in revised form 1995-07-26). EUTECTIC CARBIDE GRANULATION OF CAST Cr12 DIE STEEL[J]. 金属学报, 1995, 31(23): 523-526.
[6] LIANG Gongying;XING Jiandong Xi'an Jiaotong University. A THERMAL ANALYSIS STUDY OF Fe-Cr-Mn HEAT RESISTANT ALLOY[J]. 金属学报, 1991, 27(6): 99-103.
[7] JIANG Qichuan;LI Zhang;WANG Shoushi;HE Zhenming Jilin University of Technology; Changchun associate professor;Faculty of foundary Jilin University of Technology;Changchun 130025. BEHAVIOUR OF Ti IN AS-CAST MEDIUM MANGANESE AUSTENITIC STEEL[J]. 金属学报, 1990, 26(4): 130-134.
No Suggested Reading articles found!