Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (22): 465-467    DOI:
Current Issue | Archive | Adv Search |
DYNAMICS OF CuO/Al IN SITU COMPOSITE
KOU Shengzhong; (Faculty of Foundry; Gansu University of Technology; Lanzhou 730050)DING Yutian; XU Guangji; HAO Yuan(Gansu University of Technology; Lanzhou 730050)
Cite this article: 

KOU Shengzhong; (Faculty of Foundry; Gansu University of Technology; Lanzhou 730050)DING Yutian; XU Guangji; HAO Yuan(Gansu University of Technology; Lanzhou 730050). DYNAMICS OF CuO/Al IN SITU COMPOSITE. Acta Metall Sin, 1995, 31(22): 465-467.

Download:  PDF(235KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An Al2O3 particle reinforced aluminium matrix composite-CuO/Al reaction synthetic in situ composite has been prepared at lower temperature. Heat response of synthectic reaction and microstructure of composite were observed by thermal analysis and scanning electron microscopy.
Key words:  in situ composite      aluminium alloy      reaction synthesis     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I22/465

1小桥真,长隆郎.轻金属,1992;42:1382LusterJW,MaterSciTechnol,1993;9:85
[1] CHEN Junzhou, LV Liangxing, ZHEN Liang, DAI Shenglong. Precipitation Strengthening Model of AA 7055 Aluminium Alloy[J]. 金属学报, 2021, 57(3): 353-362.
[2] Fenjun LIU, Li FU, Haiyan CHEN. Microstructures and Mechanical Properties of Thin Plate Aluminium Alloy Joint Prepared by High Rotational Speed Friction Stir Welding[J]. 金属学报, 2017, 53(12): 1651-1658.
[3] Wei GU,Jingyuan LI,Yide WANG. EFFECT OF GRAIN SIZE AND TAYLOR FACTOR ON THE TRANSVERSE MECHANICAL PROPERTIES OF 7050 ALUMINIUM ALLOY EXTRUSION PROFILE AFTER OVER-AGING[J]. 金属学报, 2016, 52(1): 51-59.
[4] Chao YANG,Jijie WANG,Zongyi MA,Dingrui NI,Mingjie FU,Xiaohua LI,Yuansong ZENG. FRICTION STIR WELDING AND LOW-TEMPERATURE SUPERPLASTICITY OF 7B04 Al SHEET[J]. 金属学报, 2015, 51(12): 1449-1456.
[5] WANG Bo, WANG Xiaojiao, SONG Hui, YAN Jujie, QIU Tao, LIU Wenqing, LI Hui. STRENGTHENING EFFECTS OF MICROSTRUCTURE EVOLUTION DURING EARLY AGEING PROCESS IN Al-Mg-Si ALLOY[J]. 金属学报, 2014, 50(6): 685-690.
[6] ZHANG Yanbin, ZHANG Limin, ZHANG Jiwang, ZENG Jing. EFFECT OF ANODIZING TREATMENT ON BENDING FATIGUE PROPERTIES OF 2014-T6 ALUMINIUM ALLOY[J]. 金属学报, 2014, 50(6): 715-721.
[7] SHENG Hai, DONG Chaofang, XIAO Kui, LI Xiaogang. LOCALIZED ELECTROCHEMICAL CHARACTERIZATION OF HIGH STRENGTH ALUMINIUM ALLOY AT THE CRACK TIP IN 3.5NaCl SOLUTION[J]. 金属学报, 2012, 48(4): 414-419.
[8] JIA Xiaojiao ZHANG Jun SU Haijun SONG Kan LIU Lin FU Hengzhi. MICROSTRUCTURES AND MECHANICAL PROPERTIES OF Al2O3–BASIC EUTECTIC IN SITU COMPOSITES DIRECTIONALLY SOLIDIFIED BY LASER FLOATING ZONE REMELTING[J]. 金属学报, 2012, 48(12): 1479-1486.
[9] WANG Guan LIN Xiaoqun. EFFECT OF COLD DEFORMATION ON THE CORROSION BEHAVIOUR OF Mn–CONTAINING ALUMINIUM ALLOY TUBE[J]. 金属学报, 2011, 47(3): 361-366.
[10] ;. Microstructural morphology and irregular eutectic growth of directionally solidified Al2O3/YAG eutectic in situ composite[J]. 金属学报, 2008, 44(4): 457-462 .
[11] Zhou Qing. EFFECTS OF GRAIN SIZE AND THICKNESS ON CREEP DEFORMATION OF ALUMINIUM THIN FOILS WITH MESO--SCALE[J]. 金属学报, 2008, 44(3): 336-340 .
[12] Wei-Xing YAO. Gigacycle Fatigue Life Distribution of Aluminum Alloy LC4CS[J]. 金属学报, 2007, 43(4): 399-403 .
[13] LIU Wenhui; LIU Yangai; XONG Shoumei; LIU Baicheng; Y. Matsumoto; M. Murakami. Comparative Study of the Cavity Pressure of Magnesium Alloy and Aluminium Alloy During Die Casting Process[J]. 金属学报, 2005, 41(1): 103-.
[14] ZHANG Zheng; SONG Shizhe; MO Shufen. EIS CHARACTERISTIC OF LY12CZ ALLOY WITH DIFFERENT EXFOLIATION CORROSION GRADES IN 0.1 mol/L NaCl SOLUTION[J]. 金属学报, 2004, 40(7): 754-758 .
[15] MA Shuwei; ZHENG Yunrong(Beijing Institute of Aeronautical Materials; Beijing 100095)DU Wei; WEI Pengyi; LI Jianguo; FU Hengzhi(The State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072). MICROSTRVCTURE AND SOLIDIFICATION BEHMIOUR OF Ni_3Al/Ni_7Hf_2 EUTECTIC ALLOY[J]. 金属学报, 1998, 34(3): 237-241.
No Suggested Reading articles found!