| EXPERIMENTAL MODELLING FOR RHEOLOGICAL PROPERTIES OF CAST STEEL |
| LI Defu;LIN Bainian; YAN Yonggui; AN Geying (Harbin Institute of Technology;Harbin 150001)(Manuscript received 1994-08-29; in revised form 1995-02-27) |
|
Cite this article:
LI Defu;LIN Bainian; YAN Yonggui; AN Geying (Harbin Institute of Technology;Harbin 150001)(Manuscript received 1994-08-29; in revised form 1995-02-27). EXPERIMENTAL MODELLING FOR RHEOLOGICAL PROPERTIES OF CAST STEEL. Acta Metall Sin, 1995, 31(21): 389-393.
|
|
|
Abstract The rheological properties of cast steel in the range of liquid state and solid liquid coexistence region have been examined under the modified test equipment for rheological properties of superalloy, particularly with refractory fittings. The γ─t curves at various temperatures were plotied so as to propose their mechanical model and the constitutive equation. The inherent correlation between the rheological propertics of alloy and the structural change of steel during solidification together with the action among particles was analyzed.Correspondeni: (LI Defu, Deparment of Malerial Science and Technology, Harbin Institute of Technology.Harbin 150001)
|
|
|
| 1林柏年.铸造流变学.哈尔滨:哈尔滨工业大学出版社,1992:321979:2833刘驰.铝铜合金准固态力学行为和凝固过程应力、应变及热裂纹数值模拟.哈尔滨工业大学博士学位论文,19874下地光雄[日].液态金属,北京:科学出版社,1987:53` |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|