DESCRIMINATION OF D88 STRUCTURE OF INTER-METALLIC COMPOUNDS BY SELF-ORGANIZATION ARTIFICIAL NEURAL NETWORK
CAI Yudong; XU Weijie; CHEN Nianyi(Shanhai Institute of Metallurgy; ChineseA cademy of Sciences; Shanhai 200050)
Cite this article: 

CAI Yudong; XU Weijie; CHEN Nianyi. DESCRIMINATION OF D88 STRUCTURE OF INTER-METALLIC COMPOUNDS BY SELF-ORGANIZATION ARTIFICIAL NEURAL NETWORK. Acta Metall Sin, 1995, 31(18): 280-283.

Download:  PDF(291KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Kohonen′s self-organization neural network is presented to discriminate D88 structure of inter-metallic compounds. After the research for 65 compounds, the results indicated that the performance of the network is good, and therefore it might be referred as an effective assistant technique for analysis of structure of compounds.

Key words:   inter-metallic compound      D88 structure      artificial neural network      Kohonen′s self-organization model     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I18/280

1Hecht-NielsenR.In:Hecht-NielsenRed.,Theory of the BackpropagationNeuralNetwork,IntJointConfonNeuralNetwork,WashingtonDC:MIT,1989:25 2LippmannRP.IEEETransAcoustSpeechSigualProcess,1987;35(1):4 3尹红风,戴汝为.模式识别与人工智能,1990;3(1):1 4ChenNY.XuHua.Scientis.1981:24:1528
[1] HOU Jieshan, ZHOU Lanzhang, GUO Jianting, YUAN Chao. APPLICATION OF ARTIFICIAL NEURAL NETWORK FOR PREDICTION OF SUPERPLASTIC  BEHAVIOUR IN NiAl ALLOYS[J]. 金属学报, 2013, 49(11): 1333-1338.
[2] YU Hui KIM Youngmin YU Huashun YOU Bongsun MIN Guanghui. HOT DEFMATION BEHAVIOR AND HOT WORKABILITY OF Mg-Zn-Zr-Ce ALLOY[J]. 金属学报, 2012, 48(9): 1123-1131.
[3] LI Xincheng; CHEN Guang; ZHU Weixing; WANG Yun; ZHANG KAihua; WANG Jianmin. Intelligent Expert System Used in Gear Material Selection and its Heat Treatment[J]. 金属学报, 2004, 40(10): 1051-1054 .
[4] ZHANG Zhaochun; WU Zhu; LI Chonghe; QIN Pei; CHEN Nianyi(Shanghai Institute of Metallurgy; The Chinese Academy of Sciences; Shanghai 200050)Correspondent: WU Zhu; Tel: (021)62511070-8932; Fax: (021)62513510. APPLICATION OF PATTERN RECOGNITION AND ARTIFICIAL NEURAL NETWORK TO IMPROVE THE MECHANICAL PROPERTIES OF CYLINDER BLOCK CAST OF AUTOMOBILE ENGINE[J]. 金属学报, 1998, 34(10): 1068-1072.
[5] GUO Jin; LI Chonghe; QIN Pei; ZENG Wenming; CHEN Nianyi(Shanghai Institute of Metallurgy; Chinese Academy of Sciences; Shanghai 200050) (Manuscript received 1995-06-23 ; in revised form; 1995-09- 15). ARTIFICIAL NEURAL NETWORK METHOD APPLIED TO P-C RELATIONSHIPS OF AB_5-TYPE HYDROGEN STORAGE ALLOYS[J]. 金属学报, 1996, 32(3): 333-33.
[6] ZHANG Peng;CUI Jianzhong;ZHANG Qizhi;DU Yunhui;FU Jiangtao;BA Limin (Northeastern University;Shenyang 110006)(Manuscript received 1996-05-21;in revised form 1996-07-11). ARTIFICIAL NEURAL NETWORKS APPLIED TO INVESTIGATION ON SOLID-LIQUID PRESSURE BONDING OF STAINLESS STEEL AND ALUMINIUM[J]. 金属学报, 1996, 32(12): 1275-1278.
[7] ZHA NG Peixin; ZHA NG Qizhi; W U Liming; SUI Zhitong(Northeasiern Unirersity.Shenyang 110006). OPTIMIZATION OF MgO-B_2O_3-SiO_2 SLAGGING USING ARTIFICIAL NEURAL NETWORK AND GENETIC ALGORITHM[J]. 金属学报, 1995, 31(18): 284-288.
[8] TANG BO; QIN Pei; LIU Miaoxiu;ZHANG Weiming;CHEN Nianyi(Shanghai institute of Metallurgy; Chinese Academy of Sciences). ARTIFICIAL NEURAL NETWORK APPLIED TO PREDICTION OF INTERMEDIATE PHASES IN MOLTEN SALT PHASE DIAGRAMS[J]. 金属学报, 1994, 30(13): 22-26.
No Suggested Reading articles found!