OPTIMIZATION OF MgO-B_2O_3-SiO_2 SLAGGING USING ARTIFICIAL NEURAL NETWORK AND GENETIC ALGORITHM
ZHA NG Peixin; ZHA NG Qizhi; W U Liming; SUI Zhitong(Northeasiern Unirersity.Shenyang 110006)
Cite this article: 

ZHA NG Peixin; ZHA NG Qizhi; W U Liming; SUI Zhitong(Northeasiern Unirersity.Shenyang 110006). OPTIMIZATION OF MgO-B_2O_3-SiO_2 SLAGGING USING ARTIFICIAL NEURAL NETWORK AND GENETIC ALGORITHM. Acta Metall Sin, 1995, 31(18): 284-288.

Download:  PDF(289KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The relation among the MgO-B2O3-SiO2 slag compositions and the efficiencies of extraction of B has been fitted and predicated by artificial neural network. The optimum composition corresponding to the highest efficiency of extraction of B was obtained using genetic algorithm. It is believed that the artificial neural network and genetic algorithm may provide a new and effective way for fitting and optimizing the process of extraction of B.

Key words:  : artificial neural network      genetic algorithm      optimization of composition      boron      MgO-B_2O_3 SiO_2 slag     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I18/284

1ZhangPeixin,SuiZhitong.MetallMaterTrans,.1995;26B:3452HopfieldJJ.ProcNatAcadSciUSA,1982;79:25543PsaltisD,SiderisA,Yamanmuya.IEEEControlSystMag,1988;8:174GishH,In:ProcIEEEIntConfonAccosties,SpeechandSignalProcessing,1990:13615BarronAR,VanStratenFW,BarronRL,In:ProcIEEEIntConfonCyberneticsandSociely,1977:7246FunahashiK.NeuralNetworks.1989:2:183
[1] Kejian LI,Zhipeng CAI,Yao WU,Jiluan PAN. Research on Austenite Transformation of FB2 Heat-Resistant Steel During Welding Heating Process[J]. 金属学报, 2017, 53(7): 778-788.
[2] Binshan YU,Sheliang WANG,Tao YANG,Yujiang FAN. BP Neural Netwok Constitutive Model Based on Optimization with Genetic Algorithm for SMA[J]. 金属学报, 2017, 53(2): 248-256.
[3] DENG Tianyong WU Di XU Yunbo ZHAO Yanfeng LIU Xianghua WANG Guodong. A NEW MATHEMATICAL METHOD CONSTITUTING HOT ROLLED TEMPERATURE OF HEAVY AND MEDIUM PLATE FOR PLAIN CARBON STEEL[J]. 金属学报, 2009, 45(1): 67-72.
[4] . Effect of boron on the microstructure and mechanical properties of as-cast TiAl alloy[J]. 金属学报, 2007, 43(5): 487-492 .
[5] ;. Effect of Solidification Condition on Structure and Properties of High Boron Iron-Base Alloy[J]. 金属学报, 2007, 43(5): 477-481 .
[6] QIU Shengtao; XIAO Lijun; LIU Jiaqi; GAN Yong. Softening Mechanism of Boron—Bearing Low--Carbon Hot Strips Produced by TSCR Route[J]. 金属学报, 2006, 42(11): 1202-1206 .
[7] TANG Bei; LIU Yongli; ZHENG Hong; LI Feng; CONG Hongtao; CHENG Huiming. MICROSCOPIC CHARACTERIZATION AND HRTEM IMAGES OF BORON NITRIDE NANOTUBES[J]. 金属学报, 2005, 41(9): 905-909 .
[8] CHEN Guosheng; JIN Xin; ZHOU Dianhua; WANG Shipu; XIE Wei; WANG Lintao. Effects of Boron Content on Boundaries Precipitates in Ni Base Alloy GH4049 and Its High Temperature Properties[J]. 金属学报, 2005, 41(6): 622-626 .
[9] LI Fan; ZHANG Dengjun; LI Baohou; LUO Shimin. Chemical Plating Nickel on the Surface of Hexagonal Boron Nitride Micro-Particles and Its Kinetic Model[J]. 金属学报, 2004, 40(2): 173-178 .
[10] WANG Yu; LIN Dongliang(T. L. Lin)(Department of Materials Science; the Open Laboratory of Education Ministry for High-Temperature Materials and Test; Shanghai Jiao Tong University; Shanghai 200030)ZHOU Yuanxin; XIA Yuanming (Department of Morden Dynamics; University of Science and Technology of China; Hefei 230026)C. C. Law (Materials and Mechanics Engineering; United Technologies Company-Pratt & Whittney 400 Main Street; East Hartford; CT 06108; U. S. A.)Correspondent: LIN Dongliang; professon Tel: (021)62812544(O); (021)62835352(H);Fax: (021)62820892; E-mail: dllin@ mail. sjtu. edu. cn.. THE EFFECT OF MINOR BORON ADDITION ON DYNAMIC TENSILE PROPERTIES OF WROUGHT Ti-47Al-2Mn-2Nb ALLOY[J]. 金属学报, 1998, 34(9): 915-918.
[11] WU Zhengan; GU Mingyuan; CHEN Yu; ZHANG Gooding (The State Key Laboratory of MMCs; Shanghai Jiaotong University; Shanghai 200030). THE INTERFACE MICROSTRUCTURE OF A B_4C_p +SiC_w/MB15 MAGNESIUM BASED COMPOSITE[J]. 金属学报, 1998, 34(4): 443-448.
[12] LI Zhiqiang;REN Dagang;LI Douxing; GUO Jianting (Laboratory of Atom Imaging of Solids; Institute of Metal Research; The Chinese Academy of Sciences;Shenyang 110015). MICROSTRVCTURAL STUDY OF INTERMETALLIC COMPOUND Ni_3Al BY AP-FIM[J]. 金属学报, 1998, 34(3): 249-254.
[13] SUI Zhitong;ZHANG Peixin(Northeastern University; Shenyang 110006). SELECTIVE PRECIPITATING BEHAVIOR OF THE BORON COMPONENTS FROM THE BORON SLAGS[J]. 金属学报, 1997, 33(9): 943-951.
[14] CUI Chuanmeng; XU Xiuguang; ZHANG Xianpeng; WANG Kuihan; HAN Weiru (Northeastern University; Shenyang 110006). EFFECT OF COMPOSITION OF B_2O_3-MgO-SiO_2-Al_2O_3-CaO SLAG SYSTEM ON PHYSICAL PROPERTIES OF MELT[J]. 金属学报, 1996, 32(6): 637-641.
[15] ZHANG Peng;CUI Jianzhong;ZHANG Qizhi;DU Yunhui;FU Jiangtao;BA Limin (Northeastern University;Shenyang 110006)(Manuscript received 1996-05-21;in revised form 1996-07-11). ARTIFICIAL NEURAL NETWORKS APPLIED TO INVESTIGATION ON SOLID-LIQUID PRESSURE BONDING OF STAINLESS STEEL AND ALUMINIUM[J]. 金属学报, 1996, 32(12): 1275-1278.
No Suggested Reading articles found!