MICROSTRUCTURAL FEATURE OF NANOCRYSTALLINE Se
ZHANG Haoyue; LU ke; HU Zhuangqi (State Key Laboratory for RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

ZHANG Haoyue; LU ke; HU Zhuangqi (State Key Laboratory for RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). MICROSTRUCTURAL FEATURE OF NANOCRYSTALLINE Se. Acta Metall Sin, 1995, 31(15): 123-128.

Download:  PDF(434KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructural feature of nanocrystalline Se (nc-Se) was investigated by using XRD and TEM. The lattice distortions were found from the quantitative XRD measurements, from which the dependence of the lattice distortions and cell volume changes on the grain sizes were obtained. and the bond lengths of the nc-Se were calculated as well. The experimental result of the lattice distortion in the nc-Se was explained in view of the crystallization micromechanism of random-coil chains folding.
Key words:  nanocrystalline material      selenium      lattice parameter      lattice distortion. cell volume     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I15/123

1GreiterH.ProgMaterSci,1989;33:2232WagnerM.PhysRev,1992;45B:6363LuK.SuiML.JMaterSciTech.,1993;9:4194LiuXD.LuK,HuZQ.NanostructuredMater,1993;2:5815LiuXD.ZhangHY,LuK,HuZQ.JPhys:CondensMatter,1994;6:L4976ZhangHY,HuZQ,LuK.NanostructuredMater,1994:inpress7ZallenR.ThePhysisofAmorphousSolids.AWiley-IntersciencePublication.1983:938UngarP,CherinP.In:CooperCWed.,ThePhysicsofSeleniumandTellurium,OxfordPergamon,1969:223
[1] NI Song, LIAO Xiaozhou, ZHU Yuntian. EFFECT OF SEVERE PLASTIC DEFORMATION ON THE STRUCTURE AND MECHANICAL PROPERTIES OF BULK NANOCRYSTALLINE METALS[J]. 金属学报, 2014, 50(2): 156-168.
[2] LIU Li, LI Ying, WANG Fuhui. ELECTROCHEMICAL CORROSION BEHAVIOR OF NANOCRYSTALLIZED MATERIALS: GROWTH OF PASSIVE FILM AND LOCAL PITTING CORROSION[J]. 金属学报, 2014, 50(2): 212-218.
[3] TIAN Sugui, WANG Xin, XIE Jun, LIU Chen, GUO Zhongge,LIU Jiao, SUN Wenru. CHARACTERISTIC AND MECHANISM OF PHASE TRANSFORMATION OF GH4169G ALLOY DURING HEAT TREATMENT[J]. 金属学报, 2013, 49(7): 845-852.
[4] ZHAO Yufei FU Yuechun HU Qingmiao YANG Rui. FIRST-PRINCIPLES INVESTIGATIONS OF LATTICE PARAMETERS, BULK MODULI AND PHASE STABILITIES OF Ti1-xVx AND Ti1-xNbx ALLOYS[J]. 金属学报, 2009, 45(9): 1042-1048.
[5] Xiaoyan SONG. CELLULAR AUTOMATON SIMULATION STUDY ON NANOGRAIN GROWTH BASED ON THERMODYNAMIC FUNCTIONS OF NANOCRYSTALLINE[J]. 金属学报, 2008, 44(4): 495-500 .
[6] SUI Manling(Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Coerespondent: SUI Manling; Fax:(024)3890488; Tel: (024)3893000-7740; E-mail: misui mail.neu.edu.cn. AN INVESTIGATUIB ON THE RECOVERY BEHMIORS OF THE LATTICE DISTORTIONS IN AN Ni_3P/Ni NANOPHASE MATERIAL[J]. 金属学报, 1998, 34(6): 650-654.
[7] LI Bolin;ZHU Min; LI Long; LUO Kanchang;LI Zuxin (South China University of Technology; Guangzhou 510641)(Manuscript received 1996-03-19; in revised form 1996-07-15). HARDENNING AND SOFTENNING EFFECTS OF Fe-Cu NANOCRYSTALLINE SUPERSATURATED SOLID SOLUTION FORMED BY MECHANICAL ALLOYING[J]. 金属学报, 1997, 33(4): 420-426.
[8] ZHANG Yun; LIN Dongliang; HUANG Jin (Shanghai Jiaotong University; Shanghai 200030). ALLOYING BEHAVIOUR OF Mg, Ca,Y, La AND Ce IN Ni_3Al[J]. 金属学报, 1997, 33(3): 259-264.
[9] LU Ke; ZHOU Fei (State Key Laboratory for RSA; Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015). RECENT RESEARCH PROGRESS ON NANOCRYSTALLINE MATERIALS[J]. 金属学报, 1997, 33(1): 99-106.
[10] LIU Zuoquan; ZHAO Heyun; LU Yusong; LI Dexiu; LI Hin; ZHANG Shubo (Yunnan Univereity; Kunming 650091)(Manuscript received 1995-11-13; in revised form 1996-04-04). CRYSTALLIZATION OF AMORPHOUS ALLOY Fe_(78)B_(13)Si_9 INDUCED BY SHOCK WAVE[J]. 金属学报, 1996, 32(8): 862-866.
[11] CHEN Da(Shanghai Jiaotong University; Shanghai;200030). A DIFFUSION MODEL IN NANOCRYSTALLINE MATERIALS[J]. 金属学报, 1995, 31(8): 340-345.
[12] PING Dehai; LI Douxing; YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). WU Xijun(Zhejiang University; Hangzhou 310014) (Manuscript received 94-06-30). ^MICROSTRUCTURE OF NANOCRYSTALLINE MATERIALS[J]. 金属学报, 1995, 31(2): 79-84.
[13] LU Ke; LIU Xuedong;ZHANG Haoyue; HU Zhuangqi(State Key Laboratory forRSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 94-05-10). LATTICE EXPANSION IN NANOCRYSTALLINE PURE Ni[J]. 金属学报, 1995, 31(2): 74-78.
[14] SUI Manling (Northeastern University;Internattonal Centre for Materials Physics.Chinese Academy of Sciences; Shenyang);LU Ke (National Laboratoryfor RSA Insti tute of Metal Research; Chinese Academy of Sciences;Shenyang). MICROSTRUCTURES OF CRYSTALLITES IN NANOCRYSTALLINE Ni-P ALLOYS[J]. 金属学报, 1994, 30(21): 413-419.
[15] SUI Manling (Northeastern University; International Centre for Materials Physics;Chinese Academy of Sciences; Shenyang);LU Ke (Institute of Meial Research; Chinese Academy of Sciences; Shenyang). INTERFACIAL EXCESS VOLUME IN NANOCRYSTALLINE Ni-P ALLOYS WITH DIFFERENT GRAIN SIZES[J]. 金属学报, 1994, 30(15): 121-125.
No Suggested Reading articles found!