Acta Metall Sin  1994, Vol. 30 Issue (18): 259-264    DOI:
Current Issue | Archive | Adv Search |
PREPARATION OF NANOCRYSTALLINE METAL POWDERS BY γ-IRRADIATION-HYDROTHERMAL TREATMENT METHOD
ZHU Yingjie; QIAN Yitai; ZHANG Manwei; CHEN Zuyao(University of Science and Technology of China; Hefei)
Cite this article: 

ZHU Yingjie; QIAN Yitai; ZHANG Manwei; CHEN Zuyao(University of Science and Technology of China; Hefei). PREPARATION OF NANOCRYSTALLINE METAL POWDERS BY γ-IRRADIATION-HYDROTHERMAL TREATMENT METHOD. Acta Metall Sin, 1994, 30(18): 259-264.

Download:  PDF(398KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The γ-irradiation-hydrothermal treatment method has been successfully used to prepare pure nanocrystalline powders of Ag(8 nm),Cu (16 nm) and Pd (10 nm). Influences of experimental conditions on Ag particle size are discussed. The complexation of cupric ion with EDTA is favourable for the preparation of nanocrystalline Cu powder. By controlling the conditions of the experiments, different shapes of Cu particles can be obtained. The process of the formation of metal particles in the solution during γ-irradiation is also discussed.
Key words:  nanocrystalline metal      γ-irradiation      hydrothermal treatment     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I18/259

1FujitaH,IzawaM,YamazikiH.Nature,1962;196:6662BelloniJ,DelcourtMO,LeclereC.NouvJChim,1982;6:5073DelcourtMO,KeghoucheN,BelloniJ.NouvJChim,1983;7:1314DeicourtMO,BelloniJ,MarignierJL,MoryC,CollexC.RadiatPhysChem,1984;23:4855MarignierJL,BelloniJ,DelcourtMO,ChevalierJP.Nature,1985;317:3446陈祖耀,陈波,钱逸泰,张曼维,杨丽,范成高.金属学报,1992;28:B1697WagnerCNJ,AquaEN.AdvX-rayAnalysis,1964;7:46@
[1] Feng LIU, Linke HUANG, Yuzeng CHEN. Concurrence of Phase Transition and Grain Growth in Nanocrystalline Metallic Materials[J]. 金属学报, 2018, 54(11): 1525-1536.
[2] Yufeng ZHENG,Yuanhao WU. Revolutionizing Metallic Biomaterials[J]. 金属学报, 2017, 53(3): 257-297.
[3] ZHANG Guilin;XU Feng;LIU Wenhong;YU Fanghua;WANG Jingcheng;SHAO Zichang Shanghai Institute of Nuclear Research; Academia Sinica; Shanghai Iron and Steel Research Institute. EFFECT OF γ-IRRADIATION ON CuZnAl SHAPE MEMORY ALLOY[J]. 金属学报, 1992, 28(3): 42-44.
No Suggested Reading articles found!