| THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2 |
| XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993) |
|
Cite this article:
XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2. Acta Metall Sin, 1994, 30(16): 150-155.
|
|
|
Abstract The discrete complex anion modle was introduced to the molten salt solutions of LiF-CaF2,NaF-CaF2-and KF-CaF2,based upon the assumption of existence of the CaF3 complex ions contained in the melts.A set of parameters were evaluated from experimental data about enthalpies of mixing and phase diagrams of the above three systems.The thermodynamic properties and phase diagrams of the melts were calculated by using the model.The results obtained were in good agreement with experimental data.Correspondent:XU Qian,(Department of Nonferrous Metallurgy,Northeastern University,Shenyang 110006)
|
|
|
| 1PeltonAD,ThompsonWT.CanJChem,1970;48:15852KarakayaI,ThompsonWT.CanMetallQ,1986;25(4):3073HongKC,KleppaOJ.JPhysChem,1978;82(14):15964KleppaOJ,WakiharaM.JInorgNuclChem,1976;38:7155KleppaOJ,HonhKC.JPhysChem,1974;78(15):14796DeadmoreDL,MachinJS.JPhysChem,1960;64:8247BukhalovaGA,SulaimankulovK,BostandzhiyouAK.RussJInorgChem,1959;4:5168IshaqueM.BullSocChimFr,1952;2:1309BarinI,KnackeO.ThermochemicalPropertiesofInorgnicSubstance.Berlin:Springer-Verlag,1973:170,362,401,516 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|