CAVITATION AND RESIDUAL STRENGTH OF AS-WARM ROLLED Al-Li-Cu-Mg-Zr ALLOY AFTER SUPERPLASTIC DEFORMATION
LIU Qing;LIU Zhengang;YAO Mei University of Science and Technology Beijing Harbin Institute of Technology
Cite this article: 

LIU Qing;LIU Zhengang;YAO Mei University of Science and Technology Beijing Harbin Institute of Technology. CAVITATION AND RESIDUAL STRENGTH OF AS-WARM ROLLED Al-Li-Cu-Mg-Zr ALLOY AFTER SUPERPLASTIC DEFORMATION. Acta Metall Sin, 1993, 29(9): 25-30.

Download:  PDF(1825KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The residual strength and relation to the cavitation of as-warm rolledAl-Li-Cu-Mg-Zr alloy have been investigated after superplastic deformation under differ-ent tensile conditions. Under certain extent of strain, the specimen deformed at a high strainrate has less cavity and higher residual strength than that at low strain rate. Whiledeformation to a large strain, the specimen deformed under test at strain rates of two-stage,i.e., at a quick one first and slow down afterward, has less cavity and higher residual strengthin comparison with that of a single stage. The relationship among residual strength, cavitationand superplastic tensile conditions has been discussed by considering the deformation-in-duced continuous recrystallization occurred during the initial stage of superplasticdeformation.
Key words:  Al-Li-Cu-Mg-Zr alloy      superplastic deformation      residual strength      cavitation     
Received:  18 September 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I9/25

1 刘庆,黄晓旭,姚枚,杨金凤.金属学报,1991;27:B414
2 Liu Qing, Yang Jinfeng, Yao Mei. Scr Metall Mater, 1991; 25: 109
3 Ash B A, Hamilton C H. Scr Metall, 1988; 22: 277
4 Liu Qing, Yang Jinfeng, Yao Mei. Scr Metall Mater, 1991; 25: 115
5 Liu Qing, Huang Xiaoxu, Yao Mei. J Mater Sci Lett. 1991; 10: 779
6 Liu Qing, Huang Xiaoxu, Yao Mei. Acta Metall Mater, 1992; 40: 1753
7 Liu Qing, Huang Xiaoxu, Yao Mei. Scr Metall Mater, 1991; 25: 387
8 Pilling J, Geary B, Ridley N. In: McQueen H J, Bailon J P, Dickson J I, Jonas J J, Akben MG eds., Strength of Metals and Alloys, Proc ICSMA 7, Montreal, Canada, 12--16 August, 1985, Pergamon Press, 1986: 2065O
[1] LIU Haixia, CHEN Jinhao, CHEN Jie, LIU Guanglei. Characteristics of Waterjet Cavitation Erosion of 304 Stainless Steel After Corrosion in NaCl Solution[J]. 金属学报, 2020, 56(10): 1377-1385.
[2] Yanxin QIAO,Shuo WANG,Bin Liu,Yugui ZHENG,Huabing LI,Zhouhua JIANG. SYNERGISTIC EFFECT OF CORROSION AND CAVITATION EROSION OF HIGH NITROGEN STAINLESS STEEL[J]. 金属学报, 2016, 52(2): 233-240.
[3] ZHANG Ru, SHEN Hanjie, ZHANG Yaqin, LI Dongliang, LI Yanjia, YONG Xingyue. SURFACE LAYER NANO-MECHANICAL RESPONSES TO INTERACTION BETWEEN CAVITATION AND ELECTROCHEMICAL CORROSION[J]. 金属学报, 2013, 49(5): 614-620.
[4] LU Shulin WU Shusen DAI Wei AN Ping MAO Youwu. PREPARATION OF SEMISOLID 5052 ALUMINUM ALLOY SLURRY BY INDIRECT ULTRASONIC VIBRATION[J]. 金属学报, 2011, 47(5): 634-640.
[5] LIU Shihan CHEN Darong. MECHANICS MECHANISM OF DUPLEX STEEL CAVITATION DAMAGE[J]. 金属学报, 2009, 45(5): 519-526.
[6] JIANG Shengli; ZHENG Yugui; YAO Zhiming. Damage Behavior of 20SiMn Low Alloy Steel in Slurry with Different Particle Sizes[J]. 金属学报, 2004, 40(2): 163-167 .
[7] YE Wujun;FENG Di;CHEN Beijing;LUO Heli (Central Iron and Steel Research institute; BeiJing 100081). EFFECT OF METALLURGICAL FACTORS ON THE RESISTANCE OF CAVITATION EROSION OF Ni_3Al BASED ALLOYS[J]. 金属学报, 1998, 34(11): 1163-1166.
[8] LIU Yi;LI Dingqiang; LIN Dongliang(Shanghai Jiaotong University;Shanghai 200030) (Manuscript received 1995-06-28;in revised form 1995-10-12). DISLOCATION FEATURES IN FeAl ALLOY AFTER SUPERPLASTIC DEFORMATION[J]. 金属学报, 1996, 32(3): 225-230.
[9] SUN Fusheng;MA Jimin;CAO Chunxiao(Institute of Aeronautical Materials; Beijing). MICROSCOPIC OBSERVATION OF SUPERPLASTIC DEFORMATION IN A Ti_3AI ALLOY[J]. 金属学报, 1994, 30(22): 465-470.
[10] LIU Qing; YANG Wangyue; CHEN Guoliang (University of Science and Technology Beijing); WU Yiqin (Northwest Institute of Nonferrous Metal Research; Xi'an). SUPERPLASTIC DEFORMATION OF Ti-12Co-5Al ALLOY[J]. 金属学报, 1994, 30(17): 223-228.
[11] ZHANG Lichun;HE Anqiang;WU Yukun;YE Hengqiang;ZHANG Yongchang Laboratory of Atomic Imaging of Soids; Institute of Metal Research; Acadedia Sinica; Shenyang Laboratory of Microcrystal; Institute of Metal Research; Academia Sinica; ShenyangInstitute;of metal Research;Academia Sinica;Shenyang 110015. STRUCTURAL RELATIONSHIP BETWEEN Z AND T PHASES IN RAPIDLY SOLIDIFIED Al-Li-Cu-Mg-Zr ALLOY[J]. 金属学报, 1993, 29(8): 10-14.
[12] ZHENG Qiguang;LI Jiarong;LI Zaiguang Huazhohg University of Science and Technology; Wuhan; HU Weiguang PLA Unit No. 38609; TIAN Hongye PLA Factory No. 4808. EFFECT OF LASER TREATMENT ON CAVITATION EROSION RESISTANCE OF DIESEL CYLINDER[J]. 金属学报, 1991, 27(3): 116-120.
[13] JIANG Xinggang;CUI Jianzhoug;MA Longxiang Northeast University of Technology; Shenyang Box 317; Northeast University of Technology; Shenyang 110006. FRACTAL DIMENSION OF CAVITIES SHAPE CHANGES DURING SUPERPLASTIC DEFORMATION OF HIGH STRENGTH Al ALLOY 7475[J]. 金属学报, 1990, 26(4): 144-147.
[14] CUI Jianzhong;MA Longxiang Northeast University of Technology; ShenyangDepartment of Metals Forming;Northeast University of Technology; Shenyang. GRAIN SHAPE EFFECT IN SUPERPLASTIC DEFORMATION[J]. 金属学报, 1988, 24(4): 354-361.
[15] CUI Jianzhong;MA Longxiang Northeast University of Technology; ShenyangCUI Jianzhong Lecturer;P.O.Box 317;Northpast Uninersity of Technology;Shenyang. CHARACTERISTIC PARAMETERS IN SUPERPLASTIC DEFORMATION[J]. 金属学报, 1988, 24(1): 92-96.
No Suggested Reading articles found!