| EFFECT OF LIQUID FLOW ON PRIMARY ARM SPACINGS OF CONSTRAINED COLUMNAR CRYSTALS |
| LIU Shan;LU Deyang;HUANG Tao;ZHOU Yaohe National Lab of Solidification Processing; Northwestern Polytechnical University; Xi'an lecturer;National Laboratory of Solidification Processing;Northwestern Polytechnical University; Xi'an; 710072 |
|
Cite this article:
LIU Shan;LU Deyang;HUANG Tao;ZHOU Yaohe National Lab of Solidification Processing; Northwestern Polytechnical University; Xi'an lecturer;National Laboratory of Solidification Processing;Northwestern Polytechnical University; Xi'an; 710072. EFFECT OF LIQUID FLOW ON PRIMARY ARM SPACINGS OF CONSTRAINED COLUMNAR CRYSTALS. Acta Metall Sin, 1993, 29(4): 1-6.
|
|
|
Abstract An experimental apparatus, which has a convection generator and anaid-heater, is developed for the study of the effect of stable laminar liquid flow on thedirectional solidification process by the use of transparent alloy SCN-2wt-% Ace. The flowis perpendicular to primary arms. By,in-situ observation and photographing at different spe-cific moments, it has been found that such a flow can cause a great change in primaryspacings of constrained columnar crystals: for cells, the spacings become smaller; but fordendrites, they become larger. The former is mainly due to the tilted growth of upstreamsidebranches, while the latter is mainly due to the coupling effect of liquid flow with solutal fieldaround dendrite tips. The faster the liquid flows, the further smaller the cells space and thefurther larger the dendrites space.
|
|
Received: 18 April 1993
|
1 Verhoven J. Metall Trans, 1971; 2: 2673 2 任忠呜,大连理工大学博士学位论文,1988 3 Okamoto T. Kishtake K. Bessho I. J Cryst Growth, 1975: 29: 131 4 黄卫东,西北工业大学博士学位论文,1989 5 Brattkus K, Davis S H. J Cryst Growth, 1988; 87: 385 6 Huang S C, Glicksman M E. Acta Metall, 1981; 29: 717 7 黄韬,鲁德洋,周尧和,西北工业大学学报,1988;6(1) :41 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|