Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (10): 1-9    DOI:
Current Issue | Archive | Adv Search |
NONPROPORTIONAL CYCLIC PLASTICITY OF NORMALIZED STEEL 16Mn
PENG Xianghe;GAO Zhihui;MA Mingtu;YAN Zaixian Chongqing University Chongqing Institute of Automobile
Cite this article: 

PENG Xianghe;GAO Zhihui;MA Mingtu;YAN Zaixian Chongqing University Chongqing Institute of Automobile. NONPROPORTIONAL CYCLIC PLASTICITY OF NORMALIZED STEEL 16Mn. Acta Metall Sin, 1993, 29(10): 1-9.

Download:  PDF(755KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An experimental investigation was carried out of the flow characteristic andhardening of normalized steel 16Mn subjected to biaxially nonproportional cyclic straining.For a fixed cyclic strain path, the steel behaves mainly cyclic softening when the amplitude ofstrain is small. While with the increase of strain amplitude, the softening disappears gradually,and even changes to cyclic hardening for certain strain path. The hardening of the steel mayrelate to the shape of strain path under nonproportional cyclic straining. Experimental resultsshow that there exists a coupling between the hardening/softening induced by strainamplitude and that by the strain path. The memory of the steel to the history ofnonproportional cyclic hardening and the validity of Lensky's hypothesis of localdeterminability were also examined.
Key words:  steel 16Mn      nonproportional cyclic straining      plastic flow      hardening     
Received:  18 October 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I10/1

1 Miller K J, Brown M W. 6th Int Conf Fracture Mech, New Delhi, 1984
2 Lamba H S, Sidebottom O M. J Eng Mater Technol, 1978; 100: 96--111
3 Ohashi Y. J Eng Mater Technol. 1985; 107:286--292
4 Tanaka E, Murakami S, Ooka M. J Mech Phys Solids, 1985; 33: 559--575
5 Tanaka E, Murakami S, Ooka M. Acta Mech. 1985; 57: 167--182
6 Doong S H. Ph.D Thesis, Univ Ilynois at Urbana, 1988
7 马鸣图,李小宁,颜在先.拉扭复合加载计算机控制程序.全国第一届MTS材料试验会议论文集,1990
8 Lensky V S. In: Lee E H, Symonds P S eds, Plasticity, Proc 2nd Symp on Naval Structures, Pergamon, Oxford, 1960: 259/
[1] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[2] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[3] LI Xiaohan, CAO Gongwang, GUO Mingxiao, PENG Yunchao, MA Kaijun, WANG Zhenyao. Initial Corrosion Behavior of Carbon Steel Q235, Pipeline Steel L415, and Pressure Vessel Steel 16MnNi Under High Humidity and High Irradiation Coastal-Industrial Atmosphere in Zhanjiang[J]. 金属学报, 2023, 59(7): 884-892.
[4] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[5] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[6] GUO Xiangru, SHEN Junjie. Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. 金属学报, 2022, 58(3): 375-384.
[7] SHEN Guohui, HU Bin, YANG Zhanbing, LUO Haiwen. Influence of Tempering Temperature on Mechanical Properties and Microstructures of High-Al-Contained Medium Mn Steel Having δ-Ferrite[J]. 金属学报, 2022, 58(2): 165-174.
[8] WU Xiaolei, ZHU Yuntian. Heterostructured Metallic Materials: Plastic Deformation and Strain Hardening[J]. 金属学报, 2022, 58(11): 1349-1359.
[9] ZHAO Yonghao, MAO Qingzhong. Toughening of Nanostructured Metals[J]. 金属学报, 2022, 58(11): 1385-1398.
[10] LI Suo, CHEN Weiqi, HU Long, DENG Dean. Influence of Strain Hardening and Annealing Effect on the Prediction of Welding Residual Stresses in a Thick-Wall 316 Stainless Steel Butt-Welded Pipe Joint[J]. 金属学报, 2021, 57(12): 1653-1666.
[11] LIU Jizhao, HUANG Hefei, ZHU Zhenbo, LIU Awen, LI Yan. Numerical Simulation of Nanohardness in Hastelloy N Alloy After Xenon Ion Irradiation[J]. 金属学报, 2020, 56(5): 753-759.
[12] WANG Shihong,LI Jian,GE Xin,CHAI Feng,LUO Xiaobing,YANG Caifu,SU Hang. Microstructural Evolution and Work Hardening Behavior of Fe-19Mn Alloy Containing Duplex Austenite and ε-Martensite[J]. 金属学报, 2020, 56(3): 311-320.
[13] Miao JIN, Wenquan LI, Shuo HAO, Ruixue MEI, Na LI, Lei CHEN. Effect of Solution Temperature on Tensile Deformation Behavior of Mn-N Bearing Duplex Stainless Steel[J]. 金属学报, 2019, 55(4): 436-444.
[14] CHEN Lei, HAO Shuo, ZOU Zongyuan, HAN Shuting, ZHANG Rongqiang, GUO Baofeng. Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation[J]. 金属学报, 2019, 55(12): 1495-1502.
[15] Kuanhui HU, Xinping MAO, Guifeng ZHOU, Jing LIU, Zhifen WANG. Effect of Si and Mn Contents on the Microstructure and Mechanical Properties of Ultra-High Strength Press Hardening Steel[J]. 金属学报, 2018, 54(8): 1105-1112.
No Suggested Reading articles found!