Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (1): 69-74    DOI:
Current Issue | Archive | Adv Search |
DETERMINATION AND CALCULATION ON Na-Hg BINARY ALLOY PHASE DIAGRAM BY EMF METHOD
SUN Chengwen;CAO Yongxu Shanghai Institute of Ceramics; Academia Sinica
Cite this article: 

SUN Chengwen;CAO Yongxu Shanghai Institute of Ceramics; Academia Sinica. DETERMINATION AND CALCULATION ON Na-Hg BINARY ALLOY PHASE DIAGRAM BY EMF METHOD. Acta Metall Sin, 1993, 29(1): 69-74.

Download:  PDF(493KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  EMF of Na
Key words:  Na-Hg alloy      phase diagram      Na-β-Al_2O_3 tube      Na-NaHg_2 cell     
Received:  18 January 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I1/69

1 Hultgren R, Desai P D, Hawkins D T, Gleiser M, Kelley K K. Selected Values of the Thermodynamic Properties of Binary Alloys, Metals Park, Ohio: ASM, 1973: 962
2 Bent H E, Forziati A F. J Am Chem Soc, 1936; 58: 2220
3 Bertlett H E, Neethling A J, Crowther P. J Chem Thermodyn, 1970; 2: 583
4 Iverson M L, Recht H L. J Chem Eng Date, 1967; 12: 262
5 Hsueh L, Bennion D N. J Electrochem Soc, 1971; 118: 1128
6 Balej J, Dousek F P, Jansta J. Collect Czech Chem Commun, 1978; 43: 3123
7 Ishiguro T, Takeda S, Tamaki S. J Phys F, 1982; 12: 845
8 孙成文,郭祝昆,曹佳弟.应用科学学报,1983;1:43
9 孙成文,曹咏絮.应用科学学报,待发表
10 孙成文,曹佳弟.分析化学,1980;8:411
11 孙成文,曹佳弟.计量技术,1983;(5) :8
12 孙成文,曹咏絮.计量学报,1985;6:149
13 Jha I S, Singh R N, Srivastava P L, Mitra N R. Philos Mag, 1990; B61: 15
14 Hansen M. Constitution of Binary Alloys, New York. McGraw-Hill, 1958; 825
15 Schuhmann H, Sauerwald F. Z Anorg Allg Chem, 1962; 317: 2041
[1] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[2] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[3] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[4] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[5] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
[6] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[7] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[8] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
[9] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[10] YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
[11] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[12] YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.
[13] WAN Jinglong(Anhui Institute of Technology; Hefei); BI Qinghua(Shanghai University of Science and Technology). Gd-CoAl VERTICAL SECTION OF Gd-Co-Al PHASE DIAGRAM[J]. 金属学报, 1994, 30(17): 204-207.
[14] XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2[J]. 金属学报, 1994, 30(16): 150-155.
[15] SHEN Jianyun(General Research Institute for Non-Ferrous Metals;Beijing);CHATILLON C(Laboratoire de Thermodynamique et Physico-chimie Metallurgiques;Fracne)(Manuscript received 16 June;1993). THERMODYNAMICS OF Ga-In-As SYSTEM UNDER LATTICE DEFORMATION[J]. 金属学报, 1994, 30(16): 145-149.
No Suggested Reading articles found!