Please wait a minute...
Acta Metall Sin  1992, Vol. 28 Issue (7): 85-89    DOI:
Current Issue | Archive | Adv Search |
PREFERRED ORIENTATION OF DEPOSITED TiC COATING ON STEEL BY CVD
GUO Chengyan (Jilin Institute of Technology; Changchun); GOTO Takashi; HIRAI Toshio (Tohoku University; Japan)
Cite this article: 

GUO Chengyan (Jilin Institute of Technology; Changchun); GOTO Takashi; HIRAI Toshio (Tohoku University; Japan). PREFERRED ORIENTATION OF DEPOSITED TiC COATING ON STEEL BY CVD. Acta Metall Sin, 1992, 28(7): 85-89.

Download:  PDF(1100KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Investigation was made of the deposition rate, surface morphology and crystal preferred orientation of the dense TiC coating onto austenitic stainless steel in relation with CH_4/TiCl_4 mole ratio and temperature adopted in CVD processing. When the CH_4/TiCl_4 ratio is low or high, their preferred orientation may be (220) or (200), respectively, which is mainly dependent on the equilibrium concentration of active carbon in vapour phase.
Key words:  TiC coating      preferred orientation      deposition rate      surface morphology     
Received:  18 July 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I7/85

1 Ruppert W, Muenster A. US Pat. 2,962, 1954: 388
2 Takahashi T, Sugiyama K, Tomita K. J Electrochem Soc, 1967; 114: 1230
3 Nickl J J, Reiche M, Vesper R. In: Glaski F A ed., Proc 3rd Int Conf on Chemical Vapour Deposition, Electrochemical Society, Princetown, 1972: 369
4 Steinmann P A, Hintermann H E. J Vac Sci Technol, 1985; A 3: 2394
5 Kim D G, Yoo J S, Chun J S. J Vac Sci Technol, 1986; A4: 219
6 Yoon S G, Kim H G, Chun J S. J Mater Sci, 1987; 22: 2629
7 Schintlmeister W, Pacher O, Pfaffinger K, Raine T. J Electrochem Soc, 1976; 123: 924
8 Vuorinen S, Horsewell A. J Met Sci, 1982; 17: 589
9 Ljungqvist R. In: Glaski F A ed., Proc 3rd Int Confon Chemical Vapour Deposition, Electrochemical Society, Princetown, 1972: 363
10 伊藤秀章,榷田正夫,松山幸三.金属表面技术,1984;35:590
11 Ruppert W. In: Glaski F A ed., Proc 3rd Int Confon Chemical Vapour Deposition, Electrochemical Society, Princetown, 1972: 340
12 Lotgering F K. J Inorg Nucl Chem, 1959; 9: 113
[1] LIU Haixia, CHEN Jinhao, CHEN Jie, LIU Guanglei. Characteristics of Waterjet Cavitation Erosion of 304 Stainless Steel After Corrosion in NaCl Solution[J]. 金属学报, 2020, 56(10): 1377-1385.
[2] LIU Yin, LIU Tie, WANG Qiang, WANG Huimin, WANG Li, HE Jicheng. EFFECT OF HIGH MAGNETIC FIELD ON CRYSTAL ORIENTATION, MORPHOLOGY AND MAGNETOSTRICTION OF TbFe2 AND Tb0.27Dy0.73Fe1.95 ALLOYS DURING HEAT TREATMENT PROCESS[J]. 金属学报, 2013, 49(9): 1148-1152.
[3] LIU Qinghua,HUANG Yujin,LIU Jian,HU Qiaodan,LI Jianguo . MICROSTRUCTURE AND CRYSTAL ORIENTATION OF THE STEADY GROWTH ZONE IN THE DIRECTION ALLY SOLIDIFIED Ni-Fe-Ga-Co MAGNETIC SHAPE MEMORY ALLOYS[J]. 金属学报, 2013, 29(4): 391-398.
[4] LIU Yang, XIANG Wei, WANG Boyu. EFFECT OF IRRADIATION WITH PULSED ION BEAM ON THE MICROSTRUCTURE OF TiH2[J]. 金属学报, 2013, 49(10): 1269-1274.
[5] LIANG Yonghuang MAN Ruilin. PREPARATION AND CHARACTERIZATION OF ORGANIC HYBRID FILMS ON THE SURFACE OF Al TUBES[J]. 金属学报, 2010, 46(12): 1522-1528.
[6] MA Tianyu; YAN Mi; WANG Qingwei. Homogeneity of Magnetostriction of Tb--Dy--Fe—Co<110> Oriented Alloy Rod[J]. 金属学报, 2007, 43(7): 688-692 .
[7] Hua Xie. The preferred orientation and microstructure changes in directionally solidified Co-Ni-Ga ferromagnetic shape memory alloys[J]. 金属学报, 2007, 43(4): 417-421 .
[8] . [J]. 金属学报, 2007, 43(10): 1043-1047 .
[9] Jian Li; Jie Zhu. PREPARATION OF Cu-In FILM BY ELECTRODEPOSITION UNDER CONSTANT CURRENT[J]. 金属学报, 2006, 42(6): 667-672 .
[10] YU Ligen(State Key Lab. for Powder Metallurgy; Central South University of Technology; Chungsha 410083)HE Jiawen; B. C.Hendrix(State Key Lab. for Mechanical Behavior of Materials; Xi'an Jiaotong University; Xi'an 710049)Correspondent: YU Ligen; Tel: (0731)8826911-3630; Fad: (0731)8825755. THE EFFECT OF PREFERRED ORIENTATION ON X-RAY STRESS MEASUREMENT[J]. 金属学报, 1998, 34(6): 667-672.
[11] JIANG Chengbao (Department of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083)ZHOU Shonseng;ZHANG Maocai;WANG Run (State Key Laboratory for Advanced Metal Materials; University of Science and Technology Beijing; Beijing 100083). THE PREFERRED ORIENTATION, MICROSTRUCTURE AND MAGNETOSTOSTRION IN DIRECTIONALLX SOLIDIFIED TbDyFe ALLOYS[J]. 金属学报, 1998, 34(2): 164-170.
[12] LI Shunpu; CHEN Xichen (Institute of Physics; Chinese Academy of Sciences; Beijing 100080); O M; O POB C(AH YCCP; K 252142)(Manuscript received 94-01-31). GROWTH RULES OF EUTECTIC SYMBIOTIC REGION AND MICROSTRUCTUE OF Al-Si ALLOY[J]. 金属学报, 1995, 31(2): 47-55.
[13] KANG Zengqiao;GAI Xiuying;LI Jiabao;WANG Zhongguang State Key Laboratory for Fatigue and Fracture of Materials Institute of Metal Research; Academia Sinica; shenyang Correspondent research assistant; Institute of Metal Research; Academia Sinica; Shenyang 110015. INFLUENCE OF RESIDUAL STRESS AND SURFACE MORPHOLOGY ON FATIGUE PROPERTIES OF 60Mn STEEL[J]. 金属学报, 1992, 28(6): 40-46.
[14] SHI Nanlin;LIU Qingmin;CHANG Xinchun;QUAN Rong;XIA Fei Institute of Metal Research; Academia Sinica; Shenyang associate professor. CORRELATION BETWEEN TENSILE STRENGTH AND SURFACE MORPHOLOGY OF SiC FILAMENT[J]. 金属学报, 1990, 26(3): 153-156.
No Suggested Reading articles found!