| EFFECT OF SUBZERO TREATMENT ON MICROSTRUCTUE AND MECHANICAL PROPERTIES OF Y_2O_3-ZrO_2CREAMIC |
| Li Ying;Wang Xiaotian;Jin zhihao;Shi Guoshung Xi'an Jiaotong University Beijing Measuring and Analysing Center Correspondent Professor; Institute for Strength; of Metals Xi`an Jiaotong University; Xi`an 710049 |
|
Cite this article:
Li Ying;Wang Xiaotian;Jin zhihao;Shi Guoshung Xi'an Jiaotong University Beijing Measuring and Analysing Center Correspondent Professor; Institute for Strength; of Metals Xi`an Jiaotong University; Xi`an 710049. EFFECT OF SUBZERO TREATMENT ON MICROSTRUCTUE AND MECHANICAL PROPERTIES OF Y_2O_3-ZrO_2CREAMIC. Acta Metall Sin, 1992, 28(6): 90-94.
|
|
|
Abstract The effect of subzero treatment on the microstructure and mechanical proper-ties of Y_2O_3-ZrO_2ceramic have been investigated with TEM, X-Ray diffraction and tests ofmechanical properties. It was shown that the microstructure of 3Y-PSZ after subzero treat-ment by liquid nitrogen exhibit more longer and parallel lath of m-phase. Suitable subzerotreatment can improve the strength and toughness of Y-PSZ efficiently because of decreasingthe stability of t-phase and increasing the level of t→m transformation at an applied stress.However, when the time of subzero treatment excesses, the overaging effect may arised, whichcan decrease the strength and toughness of the material.
|
|
Received: 18 June 1992
|
1 Heuer A H. J Am Ceram Soc, 1987; 70: 689--698 2 Coyle T W, Cannon R M. Am Ceram Soc Bull, 1981; 60: 377 3 Hannink R H J. Materials Forum, 1988; 11: 43 4 Porter D L, Heuer A H. J Am Ceram Soc, 1979; 62: 298--305 5 Hannink R H J. Swain M V. J Aust Ceram Soc, 1982; 18: (2) : 53--62 6 Hughan R R. Hannink R H J. J Am Cream Soc, 1986; 69: 556 7 邓可能,金志浩,王笑天,硅酸盐学报,1990;47:336 8 Srinivasan S, Scattergood R O, Pfeiffer G, Sparks R G, J Am Ceram Soc, 1990; 73: 1421--1424 9 Excell J A, Marmach M. Am Ceram Soc Bull, 1986; 65: 1404--1407 10 Marshall D B, James M R, Porter J R. J Am Ceram Soc, 1989; 72: 218--227 11 Lange F F. J Mater Sci, 1982; 17: 255! |