Abstract Using the dissipated energy as an essential parameter, the energy dissipativestructure in process of fatigue damage of materials has been established. Throughthermodynamic analysis for irreversible energy dissipation in fatigue damage process, the heatdissipative variations in cyclic loading process as well as in a cycle have been systematically stu-died on the basis of low cycle fatigue tests and infrared measurement of self-heatingthermography. Meanwhile, the cyclic hysteresis energy and efficicent energy dissipation (storedenergy) have been proposed during fatigue damage process.
|
|
Received: 18 April 1992
|
1 童小燕,王德俊,徐灏.金属学报,1989,25:A359 2 Lemaitre J, Chobche J L. Mechanics of Solids Materials. Cambridge University Press, 1990: 65 3 童小燕,王德俊,徐灏.金属学报,1991,27:A149 4 Tung X Y, Wang D J, Xu H. Proc 9th Int Conf on Exper. Mechs. Denmark, 1990, |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|