CRACK INITIATION POINT DETERMINATION AND DYNAMIC FRACTURE TOUGHNESS FOR CHARPY PRE-CRACKED SPECIMEN
LIN Junshan;YAN Wenbin;TU Mingjing Xi'an Jiaotong University
Cite this article: 

LIN Junshan;YAN Wenbin;TU Mingjing Xi'an Jiaotong University. CRACK INITIATION POINT DETERMINATION AND DYNAMIC FRACTURE TOUGHNESS FOR CHARPY PRE-CRACKED SPECIMEN. Acta Metall Sin, 1992, 28(4): 28-33.

Download:  PDF(714KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The method to detect the crack initiation point of Charpy pre-cracked specimenunder dynamic loading was studied using strain gauge. The load-time curve and nominalstrain-time curve at the crack tip for impact testing specimens may be simultaneously measuredby twin-channel oscilloscope with high speed sampling and diskette storing. Based on the dy-namic finite element simulation of impact response of Charpy specimen, the measuring methodof dynamic fracture toughness was analysed and some problems in previous dynamic fracturetoughness measurement were discussed.
Key words:  crack initiation point      strain gauge      dynamic fracture toughness     
Received:  18 April 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I4/28

1 许昌淦,曾忠屏.金属学报,1990;26:A449
2 祝东.冶金工业部钢铁研究总院博士学位论文,1989
3 Kalthoff J F. In: Metal Handbook Ninth Edition, Vol. 8: Mechanical Testing, Metals Park, Ohio: ASM, 1985: 269
4 Kobayashi T. Int J Fract, 1983; 23: R105
5 Kobayashi T. Eng Fract Mech, 1984; 19: 49
6 Kalthoff J F. Int J Fract, 1985; 27: 227
7 林君山.西安交通大学博士学位论文.1989
8 Owen D R, Hinton E. Finite Element in Plasticity: Theory and Practice, Swansea UK: Pineridge Press, 1980
9 Ahmad J, Jung J, Barnes C R. Kanninen M F. Eng Fract Mech, 1983; 17: 235
[1] Xiangli FENG,Lei WANG,Yang LIU. STUDY ON MICROSTRUCTURE AND DYNAMIC FRACTURE BEHAVIOR OF Q460 STEEL WELDING JOINTS[J]. 金属学报, 2016, 52(7): 787-796.
[2] XU Zejian; LI Yulong; LI Na; LIU Yuanyong. EFFECT OF LOADING RATE ON MODE I DYNAMIC FRACTURE TOUGHNESS OF HIGH STRENGTH STEELS 40Cr AND 30CrMnSiNi2A[J]. 金属学报, 2006, 42(9): 965-970 .
[3] LI Qiang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)LAI Zuhan(International Centre for Material Physics; The Chinese Academy of Sciences; Shenyang 110015)MA Changxiang(College of Sciences; Northeastern University; Shenyang 110006)Correspondent: LI Qiang; Tel: (024)23843531-55659; Fax: (024)3891320; E-mail: qli imr ac.cn. A NEW ASSEMBLY AND EVALUATION OF DYNAMIC FRACTURE TOUGHNESS K_(1d) OF HIGH STRENGTH STEEL AT HIGH VELOCITY IMPACT[J]. 金属学报, 1998, 34(8): 852-857.
[4] XU Changgan;ZENG Zhongping Beijing University of Aeronautics and Astronautics. DYNAMIC FRACTURE TOUGHNESS OF ULTRA-STRENGTH STEELS FOR AIRCRAFT USE[J]. 金属学报, 1990, 26(6): 63-67.
No Suggested Reading articles found!