Abstract A mathematical relation is derived for mass transfer coefficient at pha-se interface evolving inert gas bubbles based on the character of fluid flow andmass transfer, which is checked with literature data. It shows that the mass transfercoefficient induced by inert gas bubbles is not only proportiona to the square rootof the volume rate of gas, but also related to the behaviour of gas bubbles suchas bubble size, bubble distribution density and interface area.
1 Szekely J著,彭一川,徐匡迪,樊养颐译.冶金中的流体流动现象,北京:冶金工业出版社,1985:355 2 Porter W F, Richardson F D, Subramanion K N. In: Hills A W D ed, Heat and Mass Transfer in Process Metallurgy, London; Inst Min Metall, 1967: 79 3 Subramanian K N, Richardson F D. J Iron Steel Inst, 1968; 206: 576 4 Brimacombe J K, Richardson F D. Trans Inst Min Metall. Sect. C, 1973; 82: 63 5 王渭源.金属学报,1964;7:376 6 Phillbrook W O, Kirkbride L D. Trans AIME, 1956; 206: 351 7 韩其勇.冶金过程动力学.北京:冶金工业出版社,1983:13
XUE Xiangxin;DU Hegui Northeast University of Technology; Shenyang Department of Ferrous Metallurgy;Northeast University of Technology;Shenyang;110006. OXIDATION OF Ti IN MOLTEN Cu UNDER WATERY ATMOSPHERE[J]. 金属学报, 1990, 26(1): 153-154.