| INDUCED TRANSFORMATION AND COLD WORKED HARDENING IN THREE STEELS DURING CONTACT FATIGUE |
| ZHANG Tongjun;HU Zhenhua;SHEN Guanxue;CUI Kun Huazhong University of Science and Technology; Wuhan |
|
Cite this article:
ZHANG Tongjun;HU Zhenhua;SHEN Guanxue;CUI Kun Huazhong University of Science and Technology; Wuhan. INDUCED TRANSFORMATION AND COLD WORKED HARDENING IN THREE STEELS DURING CONTACT FATIGUE. Acta Metall Sin, 1991, 27(2): 66-70.
|
|
|
Abstract Investigations were made by TEM, back scattering Mossbauer spectra,etc. to study the contact fatigue properties, to observe the microstructures beforeand after contact fatigueing and to measure the microhardness distribution beneaththe contact surface of the three leading screw steels. The martensitic transformationof retained austenite and the cold worked hardening are induced by contact stress.The effect of induced transformation and cold. worked hardening on the contactfatigue properties has been discussed. It is believed that the contact fatigue proper-ties of the steels may be improved by means of increasing the austenite content, yettheir hardness does not reduce so much.
|
|
Received: 18 February 1991
|
1 Zackay V F, Parker E R, Fahr D, Busch R. ASM Trans Q, 1967; 60: 252 2 姜秉元,邵尔玉,金属学报,1986;22: A297 3 Chen H C, Era H, Shimizu M. Metall Trans, 1989; 20A: 437 4 Fultz B, Morris J W Jr. Metall Trans, 1985; 16A: 173 5 Moore M A, Richardson R C D, Attwood D G. Metall Trans, 1972; 3: 2485 6 Snell E O, Shyne J C, Goldberg A. Metallography, 1977; 10: 299 7 Habig K H 著,严立译.材料的磨损与硬度,北京:机械工业出版社,1987:274 8 Zhang Tongjun. Hu Zhenhua, Shen Guanxue. Cui Kun. On the Contact Fatigue in Leading Screw Steel for Precise Ball Bearing, C-MRS-Internation'90 Symposium, June 18-22, 1990 9 吴家龙·弹性力学·上海:同济大学出版社,1987:320 10 Fujita K, Yoshida A. Wear, 1979; 52: 37 11 Leng Xiaogang, Chen Qing, Shao Eryu. Wear. 1988; 122: 33Y |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|