Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (2): 135-139    DOI:
Current Issue | Archive | Adv Search |
TENSILE BEHAVIOUR OF HIGHTEMPERATURE Ni_3 Al-Mo COMPOSITE
WANG Chengguo Shandong Polytechnic University; Jinan; KIKUCHI Shiomi Kyoto University; Japan
Cite this article: 

WANG Chengguo Shandong Polytechnic University; Jinan; KIKUCHI Shiomi Kyoto University; Japan. TENSILE BEHAVIOUR OF HIGHTEMPERATURE Ni_3 Al-Mo COMPOSITE. Acta Metall Sin, 1991, 27(2): 135-139.

Download:  PDF(1244KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The tensile behaviour of Ni_3Al-Mo alloy, prepared by directional soli-dification, was examined at the strain rates 3.3×10~(-3), 3.3×10~(-4) and 3.3×10~(-5) s~(-1)respectively, in the range from room temperature to 1273 K. The yield stress isfound to increase with raising of temperature, and reaches to a maximum at973 K. During tensile deformation, the Mo fibres act as retardation of dislocationmovement and restraint of plastic deformation.
Key words:  Ni_3Al-Mo alloy      fibre reinforcement      high temperature composite      tensile behaviour     
Received:  18 February 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I2/135

1 王成国,菊池潮美,兴津贵隆,小岩昌宏.材料,1990;39(7) :878
2 Tartaglia J M, Stoloff N S. Metall Trans, 1981; 12A: 1119
3 Funk W, Blank E. Metall Trans, 1988; 19A: 987
4 Sprenger H, Richter H, Nickl J J. J Mater Sci. 1976; 11: 2075
5 Nemoto M, Honda T, Nakagawa Y G, Saiga Y, Suto H. Trans Jpn Inst Met, 1980; 21: 495
6 三岛良积,岩田修一.新材料开发材料设计学.东京:社,1985:21
7 山口正治,马越佑吉.金属间化合物.东京:日刊工业新闻社,1986:29
8 Thornton P H, Davies R G, Johnston T L. Metall Trans, 1970; 1: 207
[1] YE Changjiang;LI Tiefan;SHEN.Jianian;MAO Xiaoyu;(Corrosion Science Lab.;Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 23 August; 1993;in revised form 26 October;1993). HIGH TEMPERATURE OXIDATION BEHAVIOR OF DS Ni_3Al-Mo BASE ALLOY[J]. 金属学报, 1994, 30(1): 44-48.
No Suggested Reading articles found!