Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (6): 151-155    DOI:
Current Issue | Archive | Adv Search |
A SOLUTION OF MINIMUM NORM FOR QUANTITATIVE PHASE ANALYSIS BY STANDARDLESS X-RAY DIFFRACTION
ZHAO Han;GONG Yansheng;SHEN Jingyuan;RUAN Qikuan;JIN Jialing;ZHU Hanyu Research Institute of Qiqihar Steel Works
Cite this article: 

ZHAO Han;GONG Yansheng;SHEN Jingyuan;RUAN Qikuan;JIN Jialing;ZHU Hanyu Research Institute of Qiqihar Steel Works. A SOLUTION OF MINIMUM NORM FOR QUANTITATIVE PHASE ANALYSIS BY STANDARDLESS X-RAY DIFFRACTION. Acta Metall Sin, 1990, 26(6): 151-155.

Download:  PDF(374KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new expression of quantitathe phase analysis by standardless X-raydiffraction has been derived using intensity matrix of vector modulus. The criterionof standardless X-ray diffraction analysis was suggested, so as to separate the diffra-ction pettern of every phase from that of sample. The optimal solution could beobtained by the least squares regression.
Key words:  X-ray diffraction      standardless phase analysis      least square regression     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/151

1 Radhakrishna Rao C. Indian J Statis, A, 1964; 329
2 肖明耀.实验误差估计与数据处理,北京:科学出版社,1984:167
3 Zevin L S. J Appl Crystallogr, 1977; 10: 147
4 Seber G A F,方开泰,张永光,冯士雍译.线性回归分析,北京:科学出版社,1987:333
5 Zevin L S. J Appl Crystallogr, 1979; 12: 582
6 林树智,张喜章.金属学报,1988;24;B53
7 Chung F H. J Appl Crystallogr, 1974; 7: 519
8 陆金生,邸秀萱.金属学报,1983;19:B161
9 Rozett R W, Petersen E M. Anal Chem, 1976; 48: 817
[1] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[2] LI Yizhuang,HUANG Mingxin. A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction[J]. 金属学报, 2020, 56(4): 487-493.
[3] LI Changji,ZOU Minjie,ZHANG Lei,WANG Yuanming,WANG Sucheng. High-Resolution X-Ray Diffraction Analysis of Epitaxial Films[J]. 金属学报, 2020, 56(1): 99-111.
[4] Weifeng HE, Xiang LI, Xiangfan NIE, Yinghong LI, Sihai LUO. Study on Stability of Residual Stress Induced by Laser Shock Processing in Titanium Alloy Thin-Components[J]. 金属学报, 2018, 54(3): 411-418.
[5] Yutuo ZHANG,Cong LI,Pei WANG,Dianzhong LI. IN SITU SYNCHROTRON X-RAY DIFFRACTION INVESTIGATION ON TENSILE PROPERTIES OF 9Ni STEEL[J]. 金属学报, 2016, 52(4): 403-409.
[6] Shenghua ZHANG,Pei WANG,Dianzhong LI,Yiyi LI. INVESTIGATION OF TRIP EFFECT IN ZG06Cr13Ni4Mo MARTENSITIC STAINLESS STEEL BY IN SITU SYNCHROTRON HIGH ENERGY X-RAY DIFFRACTION[J]. 金属学报, 2015, 51(11): 1306-1314.
[7] Zhao Ning. THE LIQUID STRUCTURE OF SN-CU LEAD-FREE SOLDERS[J]. 金属学报, 2008, 44(4): 467-472 .
[8] JIANG Chuanhai; WU Jiansheng; WANG Dezun. X--Ray Diffraction Analysis for the Recrystallization Behavior Of SiCw/Al Composite at High Temperature[J]. 金属学报, 2004, 40(10): 1023-1026 .
[9] WANG Huabin; HAN Jiecai; ZHANG Xinhong; DU Shanyi (Center for Composite Materials; Harbin Institute of Technology; Harbin 150001)Correspondent: WANG Huabin; lecturer;Tel: (0451)6414167; Fax: (0451)6415605. REACTION MECHANISM OF CONTINUALLY HEATING Ni AND A1 PARTICLES[J]. 金属学报, 1998, 34(9): 992-998.
[10] PAN Hongge; DU Honglin; CHEN Changpin; HAN Xiufeng; YANG Fuming (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)(Institute of Chinese Atomic Energy; Beijing 102413). STRUCTURAL CHARACTERIZATION OF THE Y_3(Fe, Mo)_(29) INTERMETALLIC COMPOUND[J]. 金属学报, 1998, 34(5): 473-482.
[11] LEI Yongquan;ZHANG Wenkui;YANG Xiaoguang;WANG Qidong (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027)LU Guanglie (Central Laboratory; Hangzhou University; Hangzhou 310028). PHASE COMPOSITION OF ZrM_2(M=Mn, V, Ni)HYDROGEN STORAGE ALLOYS[J]. 金属学报, 1998, 34(1): 45-50.
[12] WANG Fengping;WANG Peixuan;FANG Zhengzhi (University of Science and Technology Beting; Beting 100083); CUI Mingqi;JIANG Xiaoming; MA Hong; (Institute of High Energy Physics; Chinese Academy of Sciences; Beijing 100039). THE INTERFACIAL ANALYSIS OF MO/SiO_2 MULTILAYERS MIRROR FOR SOFT X-RAY[J]. 金属学报, 1997, 33(7): 737-741.
[13] YIN Xiaoying;WANG Yingang;TANG Ning;YANG Fuming(State Key Laboratory of Magnetism; Institute of Physics; Chinese Academy of Sciences; Beijing 100080)(Chinese People's Public Security University; Beijing 100038). CRYSTAL STRUCTURE AND MAGNETIC PROPERTIES OF Y_2Fe_(17-x)Mn_x[J]. 金属学报, 1997, 33(5): 539-542.
[14] WANG Fengping;CUI Mingqi; WANG Peixuan; FANG Zhengzhi University; of Science and Technology Beijing; Beijing 100083 Institute of High Energy Physics; Chinese Academy of Sciences; Beijing 100039(Manuscript received 1995-10-04). STUDY OF MULTILAYER INTERFACE ROUGHNESS BY LOW-ANGLE X-RAY DIFFRACTION[J]. 金属学报, 1996, 32(7): 774-778.
[15] GAI Hiuying; LI Jiabao; KANG Zengqiao; WANG Zhongguang (State Key Laboratory for Fatigue and Fracture of Materials;Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)ZHU Yongping; LI Chao (Shenyang Polytechnical University; Shenyang 110023). MECHANICAL PROPERTIES OF SHOT PEENED SURFACE FOR STEEL 60Mn[J]. 金属学报, 1996, 32(6): 605-610.
No Suggested Reading articles found!