Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (5): 131-136    DOI:
论文 Current Issue | Archive | Adv Search |
STRUCTURE AND FERROMAGNETIC RESONANCE OF METAL Fe/Cu SUPERLATTICES
BI Siyun;MA Xiaoding;SONG Ruitian;MEI Liangmo;ZHAO Jiangao;GUO Yicheng Shandong University; Jinan
Cite this article: 

BI Siyun;MA Xiaoding;SONG Ruitian;MEI Liangmo;ZHAO Jiangao;GUO Yicheng Shandong University; Jinan. STRUCTURE AND FERROMAGNETIC RESONANCE OF METAL Fe/Cu SUPERLATTICES. Acta Metall Sin, 1990, 26(5): 131-136.

Download:  PDF(930KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Metal Fe/Cu superlattice films deposited on glass substrates were pre-pared by a dc-magnetron sputtering system. The modulated structures and crystalstructures of films were examined by X-ray diffraction and TEM. The magneticproperties were studied by ferromagnetic resonance and vibrating sample magnetome-ter. The noval results show that the magnetic coupling between the neighbouringFe layers existed and affected the magnetic properties of superlattices.

Key words:  superlattice      ferromagnetic resonance      interface      spin-wave resonance     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/131

1 Shin S C, Cofield M L, Nuttall R H D. J Appl Phys, 1987; 61: 4326
2 Krishnan R, Sakakima H, Cochran J F, Heinrich B, Myrtle K, Qiao R W, Patcon C E. J Magn Magn Mater, 1987; 67: 88
3 Kozono Y, Komuro M, Narishige S, Hanazono M, Sugita Y. J Appl Phys, 1987; 61: 4311
4 Ueda Y, Takahashi M. J Magn Magn Mater, 1988; 71: 212
5 Ma X D, Yang L Y, Zhao J G, Guo H Q. J Magn Magn Mater, 1989; 80: 347
6 Pechan M J, Salamon M B, Schuller I K. J Appl Phys, 1985; 57: 3678
7 Layadi A, Lee J-W, Artman J O. J Appl Phys, 1988; 63: 3808
8 Puszkarski H. Prog Surf Sci, 1979; 9: 191
9 Kittel C. Phys Rev, 1958; B110: 1295
10 Wigen P E, Kooi C F, Shanabarger M R, Cummings U K, Baldwin M E. J Appl Phys, 1963; 34: 1157
11 Portis A M. Appl Phys Lett, 1963; 2: 69
12 McKnight S W, Vittoria C. Phys Rev, 1987; B36: 8574
13 Ramakrishna B L. Lee C H, Cheng Y, Stearns M B. J Appl Phys, 1987; 61: 4290

[1] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[2] LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng. Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance[J]. 金属学报, 2023, 59(3): 349-370.
[3] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[4] ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang. Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface[J]. 金属学报, 2023, 59(11): 1523-1532.
[5] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[6] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[7] LU Lei, ZHAO Huaizhi. Progress in Strengthening and Toughening Mechanisms of Heterogeneous Nanostructured Metals[J]. 金属学报, 2022, 58(11): 1360-1370.
[8] HU Biao, ZHANG Huaqing, ZHANG Jin, YANG Mingjun, DU Yong, ZHAO Dongdong. Progress in Interfacial Thermodynamics and Grain Boundary Complexion Diagram[J]. 金属学报, 2021, 57(9): 1199-1214.
[9] ZHAO Yuhong, JING Jianhui, CHEN Liwen, XU Fanghong, HOU Hua. Current Research Status of Interface of Ceramic-Metal Laminated Composite Material for Armor Protection[J]. 金属学报, 2021, 57(9): 1107-1125.
[10] LIU Yue, TANG Pengzheng, YANG Kunming, SHEN Yiming, WU Zhongguang, FAN Tongxiang. Research Progress on the Interface Design and Interface Response of Irradiation Resistant Metal-Based Nanostructured Materials[J]. 金属学报, 2021, 57(2): 150-170.
[11] WANG Shihong, LI Jian, CHAI Feng, LUO Xiaobing, YANG Caifu, SU Hang. Influence of Solution Temperature on γ→ε Transformation and Damping Capacity of Fe-19Mn Alloy[J]. 金属学报, 2020, 56(9): 1217-1226.
[12] WANG Fuqiang, LIU Wei, WANG Zhaowen. Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells[J]. 金属学报, 2020, 56(7): 1047-1056.
[13] YU Jiaying, WANG Hua, ZHENG Weisen, HE Yanlin, WU Yurui, LI Lin. Effect of the Interface Microstructure of Hot-Dip Galvanizing High-Strength Automobile Steel on Its Tensile Fracture Behaviors[J]. 金属学报, 2020, 56(6): 863-873.
[14] ZHANG Le,WANG Wei,M. Babar Shahzad,SHAN Yiyin,YANG Ke. Fabrication and Properties of Novel Multi-LayeredMetal Composites[J]. 金属学报, 2020, 56(3): 351-360.
[15] QIN Qin, LI Cheng, HE Liu, YE Chenlong, ZANG Yong. An Investigation of Interface Bonding Strength of Bimetal Plate Based on the Optimization of Asymmetric Double Cantilever Beam Model[J]. 金属学报, 2020, 56(12): 1617-1628.
No Suggested Reading articles found!