Acta Metall Sin  1989, Vol. 25 Issue (5): 72-75    DOI:
Current Issue | Archive | Adv Search |
STRUCTURE ANALYSIS OF HOT IMPREGNATED Al-Si COATING
LI Cuiping;LIU Xingzhi;TIAN Jifeng;GAO Yunyan Institute of Metal Research; Academia Sinica; Shenyang Northeast University of Technology; Shenyang LI Cuiping; Institute of Metal Research; Academia Sinica; 110015 Shenyang
Cite this article: 

LI Cuiping;LIU Xingzhi;TIAN Jifeng;GAO Yunyan Institute of Metal Research; Academia Sinica; Shenyang Northeast University of Technology; Shenyang LI Cuiping; Institute of Metal Research; Academia Sinica; 110015 Shenyang. STRUCTURE ANALYSIS OF HOT IMPREGNATED Al-Si COATING. Acta Metall Sin, 1989, 25(5): 72-75.

Download:  PDF(977KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure and chemical composition of the hot impregnated Al-Si coat-ing on 08Al steel sheet were analysed by SEM, EPMA and X-ray diffraction. The coatingis xonstitated by three parts: the outer is an α-Al solid solution of enriched Si and γ- (Fe,Al, Si) phases; the intermediate FeAl_3 and Fe_2Al_5 phases mainly and the inner neighbouringupon the substrate mainly Fe_2Al_5 phase.
Key words:  impregnating coating      structure analysis      Al-Si impregnation     
Received:  18 May 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I5/72

1 Buehler H E. Prakt Metallogr, 1977; 14: 341--362
2 Coburn K G. Metallurgia, 1959; 60 (357) : 17--20
3 内田幸夫,藤田充,広濑祐辅.金属表面技术,1982;33:537--543
4 Larikov L N, Fal'chenko V M, Polishchuk D F, Ryabov V R, Lozovskaya A V. In: Samsonov G V ed, Protective Coatings on Metals, Vol. Ⅲ, New York: Consultants Bureau, 1971: 66--70
5 Willey L A. Metals Hand Book, Vol. Ⅷ, 8th ed, Metals Park, Ohio: ASM, 1973: 394--395
6 平野贤一,菱沼章道.日本金属学会志,1968;32:516--521
7 Ryabov V R. In: Samsonov G V ed, Protective Coatings on Metals, Vol. Ⅲ, New York: Consultants Bureau, 1971; 96--100
8 江岛辰彦,山村力,内田直人,松琦温,二阶堂胜.日本金属学会志,1980;55:316--32
No related articles found!
No Suggested Reading articles found!