EXPERIMENTAL INVERSTIGATION OF CYCLIC HYSTERESIS ENERGY OF CARBON AND ALLOY STEELS
TONG Xiaoyan;WANG Dejun;XU Hao Northeast University of Technology; Shenyang TONG Xiaoyan; P. O. Box 180; Northeast University of Technology; 110006 Shenyang
Cite this article: 

TONG Xiaoyan;WANG Dejun;XU Hao Northeast University of Technology; Shenyang TONG Xiaoyan; P. O. Box 180; Northeast University of Technology; 110006 Shenyang. EXPERIMENTAL INVERSTIGATION OF CYCLIC HYSTERESIS ENERGY OF CARBON AND ALLOY STEELS. Acta Metall Sin, 1989, 25(5): 49-53.

Download:  PDF(414KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the low-cycle fatigue tests of carbon and alloy steels, thecyclic properties of hysteresis energy and its changing rules have been analysed. Themathematical formula of cyclic hysteresis energy of the materials with different cy-clic properties have been presented. The total absorbed enerey to failure is associ-ated with the variation of cyclic hysteresis energy.
Key words:  cyclic hyteresis loop      cyclic hysteresis energy      fatigue failure life      Masing material      Non-Masing material     
Received:  18 May 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I5/49

1 Ellyin F, Kujawski D. J Pressure Vessel Tech, 1984; 106: 342
2 Jhansale H R, Topper T H. ASTM STP519, 1973: 246
3 童小燕.东北工学院硕士学位论文,1985
4 王镇.东北工学院硕士学位论文,198
[1] CHENG Guangxu;KUANG Zhenbang;LOU Zhiwen Xi'an Jiaotong UniversityDepartment of Chemical Engineering; Xi'an Jiaotong University; Xi'an 710049. LOW-CYCLIC HYSTERESIS ENERGY FOR WELDED JOINT WITH MECHANICAL HETEROGENEITY[J]. 金属学报, 1993, 29(7): 44-50.
[2] TONG Xiaoyan TUNG Xiaoyan Northwestern Polytechnical University; Xi'an; WANG Dejun;XU Hao Northeast University of Technology; Shenyang. INFRARED DETECTION OF SELF-HEATING PROCESS DURING LOW CYCLE FATIGUE DAMAGE[J]. 金属学报, 1991, 27(2): 71-74.
No Suggested Reading articles found!