EFFECT OF TEMPERING IN PULSE MAGNETIC FIELD ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF HIGH SPEED STEEL
XU Bojun;GU Nanju;YAN Dianran; YIN Fuxing Hebei Institute of Technology GU Nanju; Division of heat treatment;Helet instiute of Technclogy; Tianjin 300132
Cite this article: 

XU Bojun;GU Nanju;YAN Dianran; YIN Fuxing Hebei Institute of Technology GU Nanju; Division of heat treatment;Helet instiute of Technclogy; Tianjin 300132. EFFECT OF TEMPERING IN PULSE MAGNETIC FIELD ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF HIGH SPEED STEEL. Acta Metall Sin, 1989, 25(5): 42-48.

Download:  PDF(2259KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Using a pulse magnetic field heat treatment equipment with low me-dium intensity made by ourself, the tempering process of high speed steel W6Mo5Cr4V2 was inverstigated. It was found that the secondary hardening process andthe transformation of retained austenite for the steel were accelerated by the pulsemagnetic field, and the tempering period could reduce to half of original. It wasshown by the analyses of X-ray and electronmicroscope that the precipitation ofcarbides becomes more homogeneous and diffuse, and the tetragonality of martensiteincreases obviousely, that causes the hardness and red-hardness of the steel increas-ing. It was comfirmed by practice that undergone tempering in pulse magneticfield, the service life of centre bits, small screw taps and punches for nuts increasedby 0.4 to 1.4 times.
Key words:  magnetic heat treatment      magnetic tempering      pulse magnetic field     
Received:  18 May 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I5/42

1 #12
2 #12
3 许伯钧,谷南驹,阎殿然.河北工学院学报,1987;(2) :74
4 郭耕三.高速钢及其热处理,北京:机械工业出版社,1985
5 Zablotskiy V K, Disklich M M, Voyakin V N, Sharaban N D. Phys Met Metallogr, 1981; 50 (2) : 102=
No related articles found!
No Suggested Reading articles found!