PHASE STRUCTURE OF Ti-Cu_(1-x)-Fe_x SYSTEM
WU Tiyan;LI Jianchun Central-South University of Technology; Changsha
Cite this article: 

WU Tiyan;LI Jianchun Central-South University of Technology; Changsha. PHASE STRUCTURE OF Ti-Cu_(1-x)-Fe_x SYSTEM. Acta Metall Sin, 1989, 25(3): 12-16.

Download:  PDF(754KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phase structure of Ti-Cu_(1-x)-Fe_x with x=0.1--0.6 were investigatedby means of Mossbauer spectroscopy, X-ray diffraction and microprobe. The resultsshow that there are γ -TiCu and Ti(CuFe) Phase with CsCl type structure in thealloys of x=0.1 and 0.2. Single phase of CsCl type was found in all other allays.The solubility of Fe in γ-TiCu lattice is merely 1at.-% and the Cu content in CsCltype structure is up to 37.5at.-%.
Key words:  Ti-Cu-Fe system      phase structure      Mossbauer     
Received:  18 March 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I3/12

1 Maeland A J. Adv Chem Ser, 1978; (167) : 302
2 曾贻伟.北京师范大学学报,1985;2:29
3 Swartzendruber L J, Bennett L H. J Appl Phys, 1968; 39: 1323
4 Koizumi C J, Cathey W N. J Phys F: Metal Phys, 1980; 10: 495
S Ron M, Oswald R S, Ohring M, Rothberg G M, Polcari M R. Bull Am Phys Soc, 1976; 21: 273
6 Karlsson N. J Inst Met, 1951; 79: 391
7 Averbach B L, Cohen M. Trans AIME, 1948; 176: 4017
[1] ZHANG Zhiqiang DONG Limin YANG Yang GUAN Shaoxuan LIU Yuyin YANG Rui. INFLUENCES OF QUENCHING TEMPERATURE ON THE MICROSTRUCTURE AND DEFORMATION BEHAVIORS OF TC16 TITANIUM ALLOY[J]. 金属学报, 2011, 47(10): 1257-1262.
[2] DONG Dan-Yang; Changsheng LIU. INVESTIGATION OF HYPERFINE STRUCTURE OF LASER CLADDING Fe-Si COATING[J]. 金属学报, 2008, 44(2): 188-192 .
[3] GAO Fang; JIANG Chengbao; LIU Jinghua; XU Huibin. Effects of the Third Element Additions on Phase Constitution and Magnetostriction of Fe--Ga Alloys[J]. 金属学报, 2007, 43(7): 683-687 .
[4] . Phase Structure and Magnetostriction of B element doped[J]. 金属学报, 2006, 42(8): 830-834 .
[5] GENG Ping;ZENG Meiguang;QIAN Cunfu;CHAO Yuesheng (Sciences College; Northeastern University; Shenyang 110006). STUDY OF HYPERFINE-FIELD ON NEW HIGH STRENGTH HIGH FRACTURE TOUGHNESS STEEL G99[J]. 金属学报, 1998, 34(2): 216-220.
[6] XIE Guoqiang; CHU Fengmin. YANG Jilian; LI Wendan; ZHANG Baisheng (China Institute of Atomic Energy; P. O.Box 275(51); BeiJing 102413) (Manuscript received 1996-09-09; in revised form 1996- 11 -22). MARTENSITE IN U-10%Zr ALLOY[J]. 金属学报, 1997, 33(8): 785-790.
[7] WANG Jianqiang; ZENG Meiguang;CAO Yuesheng;ZHANG Baojin (Northeastern University; Shenyang 110006) HU Zhuangqi (State Kce Laboratory for RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1996-03-06; in revised form 1996-06-05). MICROSTRUCTURAL MOSSBAUER SPECTRUM ANALYSIS OF RAPIDLY SOLIDIFIED Al-Fe-V-Si ALLOYS[J]. 金属学报, 1997, 33(4): 359-363.
[8] WANG Chunsheng; (Department of Materials Science and Engineering; Zhejiang University; Hangzhou 310027) LEI Yongquan; YANG Xiaoguang; JIANG Jianjun; WU Jing;WANG Qidong (Zhejiang University; Hangzhou; 310027). EFFECTS OF PHASE STRUCTURES OF TiNi ON THE ELECTROCHEMICAL PROPERTIES[J]. 金属学报, 1995, 31(22): 440-444.
[9] LIU Xuedong;ZHU Jie;JIANG Jian;DING Bingzhe;WANG Jingtang Institute of Metal Research. Academia Sinica; Shenyang. STRUCTURE OF NANOCRYSTALLINE Fe-Cu-Si-B ALLOYS[J]. 金属学报, 1993, 29(9): 72-76.
[10] LUO Zhiping;ZHANG Shaoqing Institute of Aeronautical Materials; Beijing; China doctoral candidate;P.O. Box 81-4; Beijing 100095;China. MICROSTRUCTURES OF Mg-Zr, Mg-Zn AND Mg-Zn-Zr ALLOYS[J]. 金属学报, 1993, 29(4): 30-36.
[11] HUANG Jianshun; CHEN Junming (Shanghai Institute of Metallurgy; Academia Sinica). CRYSTAL STRUCTURE OF γ-Li_xFe_2O_3 WITH ELECTROCHEMICAL INSERTION OF Li[J]. 金属学报, 1992, 28(8): 77-83.
[12] CHE Guangcan Institute of Physics; Academia Sinica; Beijing; ELLNER M. Max-Planck-Institut for Metallforschung; Stuttgart; Germany. PHASE DIAGRAM OF Bi-Pb-Tl TERNARY SYSTEM[J]. 金属学报, 1991, 27(6): 152-154.
[13] ZHENG Yasgzeng;ZHANG Fucheng Yanshan University; Qinhuangdao. EFFECT OF HETEROGENEOUS DISTRIBUTION OF C AND ALLOYING ELEMENTS ON γ/α′ TRANSFORMATION IN A Fe-Mn-Cr-C ALLOY[J]. 金属学报, 1991, 27(3): 82-85.
[14] ZHANG Daoyuan;XIONG Caoshui;SUN Tianfu;WANG Zheng;HUANG Meiqing University of Science and Technology of China; Hefei. CRYSTALLOGRAPHIC SITES AND PROPERTIES OF SmFe_(10)-Co-xTi COMPOUNDS[J]. 金属学报, 1991, 27(1): 148-150.
[15] HUANG Meifen;SUN Ying;SONG Jialong;ZHAO Changyu Shanghai Research Insitute of Materials. DECELERATION OF SCALE FORMATION ON STEEL DURING HEATING BY EMULSIFIED OIL[J]. 金属学报, 1991, 27(1): 137-140.
No Suggested Reading articles found!