Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (6): 447-449    DOI:
Current Issue | Archive | Adv Search |
IN SITU OBSERVATION OF LOWER BAINITIC CARBIDES PRECIPITATION
KANG Mokuang;SUN Jialin Northwestern Polytechnic University; Xi'an Manuscript received 16 December; 1987
Cite this article: 

KANG Mokuang;SUN Jialin Northwestern Polytechnic University; Xi'an Manuscript received 16 December; 1987. IN SITU OBSERVATION OF LOWER BAINITIC CARBIDES PRECIPITATION. Acta Metall Sin, 1988, 24(6): 447-449.

Download:  PDF(892KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The lower bainitic carbides precipitation in 40CrMnSiMoV steel previouslyaustempered at 310℃ was observed in situ under high temperature stage on high voltage TEM.The typical lower bainitic carbides can precipitate from within bainitic ferrite tempered attemperature higher than isothermal transformation for certain period. It revealed that the lowerbainitic ferrite is supersaturated with C. The carbides may also precipitate from austenite, butthey have no typical feature ofthe lower bainitic carbides.
Key words:  carbide precipitation      supersaturation      lower bainitic carbide      high voltge transmission electron microscopy     
Received:  18 June 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I6/447

1 Hehemann R F, Kinsman K R, Aaronson H I. Metall Trans, 1972; 3: 1077
2 Christian J W, Edmonds D V. In: Marder A R, Goldstein J I eds., Proc Int Conf on Phase Transformations in Ferrous Alloys, TMS-AIME, 1984: 293
3 Honeycombe R W K. Metall Trans, 1976; 7A: 915
4 孙加林,马世良,康沫狂,金属学报,(待发表
[1] Yingche MA,Shuo LI,Xianchao HAO,Xiangdong ZHA,Ming GAO,Kui LIU. RESEARCH ON THE CARBIDE PRECIPITATION AND CHROMIUM DEPLETION IN THE GRAIN BOUNDARY OF ALLOY 690 CONTAINING DIFFERENT CONTENTS OF NITROGEN[J]. 金属学报, 2016, 52(8): 980-986.
[2] LI Shuo CHEN Bo MA Yingche GAO Ming LIU Kui. EFFECTS OF NITROGEN CONTENT ON MICROSTRUCTURE AND MECHANICAL PROPERTY OF ALLOY 690[J]. 金属学报, 2011, 47(7): 816-822.
[3] XU Hui;HE Kaiyuan;CHENG Lizhi (Department of Materials Science and Engineering; Northeast University; Shenyang 110006). MAGNETIC PROPERLIES AND STRUCTURE OF A MIXTURE OF α-Fe and Fe_3N DURING MECHANICAL ALLOYING PROCESS[J]. 金属学报, 1998, 34(1): 86-90.
[4] LIU Xiang; ZOU Li; HU Huosheng; ZHANG Guozhi; CHENG Lizhi (Northeastern University; Shenyang); HU Zhuangqi (State Key Laboratory of RSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang)(Manuscript received 4 April; 1994). MICROSTRUCTURE OF Sn-Bi NANOMETER POWDER PREPARED BY ELECTROHYDRODYNAMIC TECHNIQUE[J]. 金属学报, 1994, 30(23): 499-502.
No Suggested Reading articles found!