TEMPERATURE DEPENDENCE UPON VISCOSITY OF Ni-P ALLOY ON AMORPHOUS FORMATION
WANG Jingtang;PANG Dexing;DING Bingzhe;BIAN Maoshu;LI Shuling Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

WANG Jingtang;PANG Dexing;DING Bingzhe;BIAN Maoshu;LI Shuling Institute of Metal Research; Academia Sinica; Shenyang. TEMPERATURE DEPENDENCE UPON VISCOSITY OF Ni-P ALLOY ON AMORPHOUS FORMATION. Acta Metall Sin, 1988, 24(5): 444-447.

Download:  PDF(299KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The temperature dependence upon viscosity and the viscous flow of the amorph-ous state of Ni-P binary alloy have been investigated on the basis of its surface tension anddensity measured. An expansion for the temperature dependence upon viscosity of the Ni-P alloyfrom liquid to amorphous solid is derived as: η=C·exp[(B+bT~(1-1/T))/(T-T_(vs)~0)]
Key words:  Ni-P amorphous alloy      viscosity      surface tension     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/444

1 Von Gebhardt E, Becker M et al. Z Metallk, 1951; 42: 111, 1952; 43: 106, 1953; 44: 379, 1954; 45: 83, 1955; 46: 90, 1956; 47: 684
2 Mazurin O V. J Non-Cryst Solids, 1977; 25: 12
[1] Yachao SUN, Minggang ZHU, Rui HAN, Xiaoning SHI, Nengjun YU, Liwei SONG, Wei LI. Magnetic Viscosity of Anisotropic Rare Earth Permanent Films[J]. 金属学报, 2018, 54(3): 457-462.
[2] Liu CAO, Fei SUN, Tao CHEN, Zihao TENG, Yulong TANG, Dunming LIAO. Numerical Simulation of Liquid-Solid Conversion Affecting Flow Behavior During Casting Filling Process[J]. 金属学报, 2017, 53(11): 1521-1531.
[3] Weidan LI,Xiaohua TAN,Kezhi REN,Jie LIU,Hui XU. MAGNETIC VISCOSITY BEHAVIOR AND EXCHANGE INTERACTION FOR Nd2Fe14B/α-Fe NANOCOMPOSITE PERMANENT ALLOYS[J]. 金属学报, 2016, 52(5): 561-566.
[4] WANG Hongyan LIN Xin WANG Lilin MA Liang YANG Donghui HUANG Weidong. COUPLING EFFECT ON RHEOLOGY AND MICROSTRUCTURE OF SEMI-SOLID SCN-5H2O MODEL ALLOY[J]. 金属学报, 2011, 47(9): 1123-1128.
[5] LIN Ben WANG Baoshun ZHANG Maicang DONG Jianxin. RESEACH ON LUBRICATION IN HOT EXTRUSION OF G3 CORROSION RESISTANT Ni–BASED ALLOY TUBE II. Calculation and Application of Glass Lubricant Viscosity–Composition[J]. 金属学报, 2011, 47(3): 374-379.
[6] Zheng Zhou-Shun. Defects and Variation of viscosity in Powder Injection Molding Filling Process[J]. 金属学报, 2007, 43(2): 183-193 .
[7] Zhang Yanju. Rheological Behavior of Semi--solid A356 Aluminum Alloy at Steady State[J]. 金属学报, 2006, 42(2): 163-166 .
[8] . STUDY OF THE SCALING LAW FOR VISCOSITY COEFFICIENTS IN SIMPLE MELTS[J]. 金属学报, 2006, 42(12): 1262-1266 .
[9] ZHAO Yuzhen; LEI Yongping; SHI Yaowu. Modeling of the Effects of Oxygen Content on Flow Patterns in A-Tig Welding[J]. 金属学报, 2004, 40(10): 1085-1092 .
[10] CUI Chuanmeng; XU Xiuguang; ZHANG Xianpeng; WANG Kuihan; HAN Weiru (Northeastern University; Shenyang 110006). EFFECT OF COMPOSITION OF B_2O_3-MgO-SiO_2-Al_2O_3-CaO SLAG SYSTEM ON PHYSICAL PROPERTIES OF MELT[J]. 金属学报, 1996, 32(6): 637-641.
[11] SHUI Jiapeng; WANG Yulin (Laboratory of Internal Friction and Defects in Solids;Institute of Solid State Physics; Chinese Academy of Sctences; Hefei 230031). VISCOUS FLOW BEHAVIOUR OF AMORPHOUS Pd-Cu-SiALLOY[J]. 金属学报, 1996, 32(11): 1215-1220.
[12] DIA O Risheng(Panzhihua Institute of Iron and Steel Research; Panzhihua 617000). DETECTION OF SURFACE TENSION OF TITANIFEROUS SLAG AND ITS RELATION TO ION-CLUSTER STRUCTURE MODEL[J]. 金属学报, 1995, 31(18): 247-250.
[13] GUO Wenquan;WANG Jingtang Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Institute of Metal Research; Academia Sinica; Shenyang. ON THE ADOPTION OF λ_0 VALUE FOR ROSCOE'S EQUATION[J]. 金属学报, 1992, 28(4): 17-20.
[14] DIAO Risheng;WANG Xiqing;WANG Huaiyong;ZHANG Rong;DU Hegui Iron and Steel Research Institute; Panzhihua Iron and Steel Company; Northeast University of Technology; Shenyang. CORRELATION OF ION-CLUSTER STRUCTURE WITH BULK VISCOSITY AND DENSITY OF TiO_2-BEARING MOLTEN SLAG[J]. 金属学报, 1992, 28(3): 55-59.
[15] LIANG Jianduan;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang. APPLICATION OF MAXIMUM ENTROPY METHOD TO CALCULATE RDF OF Ni-P AMORPHOUS ALLOY FROM X-RAY DIFFRACTION DATA[J]. 金属学报, 1989, 25(1): 141-146.
No Suggested Reading articles found!