Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (5): 448-450    DOI:
Current Issue | Archive | Adv Search |
LIQUIDUS OF Ag-Cu-Bi SYSTEM
LIU Shuqi;SUN Wenqing Department of Chemistry; Peking University
Cite this article: 

LIU Shuqi;SUN Wenqing Department of Chemistry; Peking University. LIQUIDUS OF Ag-Cu-Bi SYSTEM. Acta Metall Sin, 1988, 24(5): 448-450.

Download:  PDF(159KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The diagram of Ag-Cu-Bi system was constructed from the investigation of 12internal sections by DTA heating as well as cooling curves in an atmosphere of dry N_2. The com-position of ternary eutectic point melting at 258℃ lies in Ag(5.0)-Cu(0.5)-Bi(94.5) at.-%.The liquiduses of Ag-Cu, Ag-Bi and Cu-Bi binaries were reinvestigated.
Key words:  Ag-Cu-Bi ternary system      liquidus     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/448

1 Hansen M. Constitution of Binary Alloys, 2nd ed., New York: McGraw-Hill, 1958: 11, 18, 30
[1] GAO Zhongtang, HU Rui, WANG Jun, YANG Jieren, LI Jinshan. EFFECT OF ELECTROMAGNETIC MELT TREATMENT NEAR LIQUIDUS ON THE FORMATION OF NON-DENDRITE MICROSTRUCTURE OF SUPERALLOY[J]. 金属学报, 2014, 50(12): 1471-1477.
[2] LIU Shuqi;YI Tao Department of Chemistry; Peking University; Beijing. LIQUIDUS OF Au-Cu-Si SYSTEM[J]. 金属学报, 1990, 26(4): 153-154.
[3] LIU Shuqi;YI Tao Department of Chemistry; Peking University. LIQUIDUS OF Ag-Cu-Ge PHASE DIAGRAM[J]. 金属学报, 1989, 25(2): 155-156.
[4] ZHENG Chaogui;JIN Jun;YE Yupu Peking University. LIQUIDUS OF NdCl_3-MgCl_2-LiCl SYSTEM[J]. 金属学报, 1989, 25(1): 147-149.
[5] QIU Yiming;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang. RULE OF SEGREGATION OF ALLOYING ELEMENTS IN CAST Ni-BASE SUPERALLOYS[J]. 金属学报, 1989, 25(1): 78-80.
No Suggested Reading articles found!