EQUILIBRATING PARTITION RATIOS OF Nb, Mn and Si BETWEEN LIQUID IRON AND MgO-SiO_2 -MnO SLAG MELTS
TANG Zhonghe;GUO Shangxing;CHEN Yongding Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

TANG Zhonghe;GUO Shangxing;CHEN Yongding Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. EQUILIBRATING PARTITION RATIOS OF Nb, Mn and Si BETWEEN LIQUID IRON AND MgO-SiO_2 -MnO SLAG MELTS. Acta Metall Sin, 1988, 24(5): 397-402.

Download:  PDF(389KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Liquid iron containing Nb, Mn and Si elements has been equili-brated with MgO-SiO_2-MnO slag melts at 1600℃ in a Mo wire-wound resistance fur-nace with a duration of 4 hours. The oxygen activities in liquid iron were mea-sured with oxygen sensors. Using the known equilibrium constants of concerningreactions and the oxygen activities in liquid iron, the components activities in theslag melts can be calculated. It was found that the partition ratios of Nb, Mn andSi have a close linear relationship with α_(FeO) in logarithmic scale. The dependenceof Nb partition ratio on mole fractions of the slag components was also obtained.
Key words:  MgO-SiO_2-MnO slag      equilibrating partition ratio     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/397

1 Janke D, Fischer W A. Arch Eisenhuttenwes. 1975; 46: 755--760
2 古隆建,唐仲和.金属学报,1985;21:A167--173
3 Sigworth G K, Elliott J F. Met Sci, 1974; 8(9) : 298--310
4 张圣弼,佟亭,王济舫,魏寿昆.金属学报,1984;20:A355
5 唐仲和,朱果灵.北京钢铁研究总院学报,1988;8(1) :37--38
6 唐仲和,单玲珍,谢效方,朱卓敏,陈永定.北京钢铁研究总院学报.1983:3(2) :149--154
7 Chipman J, Fetters K I. Trans ASM, 1941; 29: 953--967V
No related articles found!