ISOTHERMAL SECTION OF THE W-Ni-Cu SYSTEM AT 1017℃
QIU Cai'an;JIN Zhanpeng;HUANG Peiyun Central South University of Technology; Changsha
Cite this article: 

QIU Cai'an;JIN Zhanpeng;HUANG Peiyun Central South University of Technology; Changsha. ISOTHERMAL SECTION OF THE W-Ni-Cu SYSTEM AT 1017℃. Acta Metall Sin, 1988, 24(5): 403-406.

Download:  PDF(782KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The isothermal section of the W-Ni-Cu ternary system at 1017℃ wasdetermined by means of diffusion couple sepecimens, EMPA and X-ray diffrac-tion. Body-centered tetragonal Ni_4W and orthorhombic NiW but NiW_2 observedin the W-Ni binary system at this temperature. The solubility ranges of W andCu in Ni_4W are 16.95--20.51 at-% and 0--4.36 at-%, respectively. The maximumsolubility of W in γ(Ni) is 13.11 at-%
Key words:  W-Ni-Cu system      phase diagram      diffusion couple     
Received:  18 May 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I5/403

1 金展鹏.中南矿冶学院学报,1984;(1) :27--35
2 Epremian E, Harker D. Trans AIME, 1949; 185 (4) : 267--273
3 Hansen M. Constitution of Binary Alloys, New York: McGraw-Hill, 1958: 1057--1059.
4 #12
5 Elliott R P. Constitution of Binary Alloys, First Suppl, New York: McGraw-Hill, 1965: 677
6 Shunk F A. Constitution of Binaty Alloys, 2nd Suppl., New York: McGraw-Hill, 1969: 561
7 Walsh J M, Donachie M J Jr. Metall Trans, 1973; 4 (12) : 2854--2855
8 Poulesn K E, Rubaek S, Langer E W. Scr Metall, 1974; 8 (11) : 1297--1300
9 Kozma L, Labar J. In: O?tner H M ed., Plansee Seminar, Vol. Ⅰ, Reutte, Austria: Metallwerk Plansee, 1981: 237--245
[1] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[2] Chengsong LIU,Fei YE. Mechanism on Modification of MnO-SiO2-Type Oxide by Interfacial Solid-State Reaction During Heat Treatment[J]. 金属学报, 2017, 53(1): 10-18.
[3] Yu GONG, Yongchong CHEN, Dandan LIU, Yanping ZHANG, Csaba CSERHáTI, Attila CSIK. INVESTIGATION OF PERIODIC-LAYERED STRUCTURE DURING SOLID STATE REACTIONS OF Zn/CuxTiy SYSTEMS[J]. 金属学报, 2016, 52(3): 349-354.
[4] WU Changjun, ZHU Chenlu, SU Xuping, LIU Ya, PENG Haoping, WANG Jianhua. THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION[J]. 金属学报, 2014, 50(8): 930-936.
[5] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[6] . Diffusion-induced Stresses[J]. 金属学报, 2006, 42(3): 225-233 .
[7] FU Xiaoliang; LI Changrong; LI Mei; ZHANG Weijing. Determination of the Phase Equilibrium of the Ag-Ti Binary System at 980, 1100 and 1200℃[J]. 金属学报, 2005, 41(7): 691-694 .
[8] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[9] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[10] DING Jinjun;ZHAO Gang;HAO Shiming (Department of Materials Science and Engineering; School of Materials and Metallurgy; Northeastern University;Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS OF α_2(α)/γ IN THE Ti-Al-Cr TERNARY SYSTEM[J]. 金属学报, 1998, 34(2): 171-175.
[11] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
[12] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[13] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[14] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
[15] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
No Suggested Reading articles found!