Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (4): 305-308    DOI:
Current Issue | Archive | Adv Search |
RELATIONSHIP BETWEEN METASTABLE EXTENSION OF SOLID SOLUBITY OF EUTECTIC SYSTEMS AND PHASE DIAGRAM
NING Yuantao Institute of Precious Metals; Kunming
Cite this article: 

NING Yuantao Institute of Precious Metals; Kunming. RELATIONSHIP BETWEEN METASTABLE EXTENSION OF SOLID SOLUBITY OF EUTECTIC SYSTEMS AND PHASE DIAGRAM. Acta Metall Sin, 1988, 24(4): 305-308.

Download:  PDF(328KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A criterion of the metastable extension of solid solubility was propo-sed. When the eutectic concentration arm ratio parameter of an alloy, J>10, thehypereutectic extension and the metastable solid solubity limit beyond eutecticconcentration may be obtained. When J≤10, the hypoeutectic extension may be obtained. The extension parameter, C_(eq)~s/C_(eu), is directly proportional to the parameter J.Thus, it seems easy to predict the tendency of the solid solubility extension underrapid solidification on the basis of the eutectic phase diagram.
Key words:  eutectic system      solid solubility extension      phase diagram     
Received:  18 April 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I4/305

1 Anantharaman T R, Suryanarayana C. J Mater Sci, 1971; 6: 1111
2 Anantharaman T R, Ramachandrarao P, Suryanarayana C, Lele S, Chattopadhyay K. Trans India Inst Met, 1977; 30: 422
3 周新铭,靳嘉禄,宁远涛,赵钟民.金属学报,1982;18:534
4 宁远涛,郑云.金属学报,1983;19:B225
5 宁远涛.金属学报,1983;19:A346
6 宁远涛.分子科学学报,1981;1:75
7 Predel B. Acta Metall, 1966; 14: 209
8 Donald I W, Davies H A. J Non-Crystal Solids, 1978; 30: 77
9 Whang S H. Mater Sci Eng, 1983; 57: 87
10 宁远涛.周新铭,金属学报,1981;17:278
[1] GAO Xiang, ZHANG Guikai, XIANG Xin, LUO Lizhu, WANG Xiaolin. Effects of Alloying Elements on the Adsorption of Oxygen on V(110) Surfaces: A First-Principles Study[J]. 金属学报, 2020, 56(6): 919-928.
[2] ZHANG Weibin SHA Chunsheng DU Yong WEN Guanghua XIE Wen WANG Shequan. COMPUTER SIMULATIONS AND VERIFICATION OF GRADIENT ZONE FORMATION IN CEMENTED CARBIDES[J]. 金属学报, 2011, 47(10): 1307-1314.
[3] ZHANG Huawei; LI Yanxiang; LIU Yuan. Study of Metal--Hydrogen Binary Phase Diagram in Gasar Process[J]. 金属学报, 2005, 41(1): 55-.
[4] ZHANG Jian(Metallurgical Engineering School; University of Science and Technology Beijing; Beijing 100083). CONSISTENCY(OR SIMILARITY) OF THERMODYNAMIC PROPERTIES OF METALLURGICAL MELTS WITH THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(7): 742-752.
[5] Zhang Jian (Institute of Metallurgy; University of Science and Technology Beijing; Beijing 100083). CLASSIFICATION OF THERMODYNAMIC PROPERTIES OF BINARY METALLIC MELTS ACCORDING TO THEIR PHASE DIAGRAMS[J]. 金属学报, 1998, 34(1): 75-85.
[6] ZHOU Hong; WANG Jinguo; JIA Shusheng (Jilin University of Technology; Chanerhun 130025) OGIKeisaku(Kyushu Universily; Japan) (Manuscript received 1996-03-22; in revised form 1997-04- 13). SOLIDIFIED MICROSTRUCTURES AND PHASES OF HIGH SPEED STEELS CONTA1NING DIFFERENT V AND C CONTENT[J]. 金属学报, 1997, 33(8): 838-843.
[7] FANG Jianhui; TANG Yun; LI Yu; YAN Licheng; CHEN Nianyi (Shanghai University;Shanghai 201800); WANG Jiyang (Shandong University; Jinan 250012)(Manuscript received 1996-04-08; in revised form 1996-09-10). KPO_3-M0O_3 PHASE DIAGRAM[J]. 金属学报, 1997, 33(4): 395-397.
[8] ZHOU Guozhi(Kuo-Chih Chou) (University of Science and Technology Beijing;Beiing 100083). NEW GENERATION SOLUTION GEOMETRICAL MODEL AND ITS FURTHER DEVELOPMENT[J]. 金属学报, 1997, 33(2): 126-132.
[9] DING Jinjun;ZHAO Gang;HAO Shiming (Northeastern University; Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS AND INTERDIFFUSION COEFFICIENTS OF β,α ANDγIN THE Ti-Al BINARY SYSTEM[J]. 金属学报, 1997, 33(10): 1105-1109.
[10] YUAN Wenxia; MA Shulan; QIAO Hin; ZHUANG Weidong; XING Xianran;QIAO Zhiyu (University of Science and Technology Beijing; Beijing 100083)(General Institute for Non-Ferrous Metals; Beijing 100088)(Manuscript received 1995-04-28; in revised form 1995-11-05). A STUDY ON THE YCl_3-AECl_2(AE=Mg, Ca, Sr, Ba)BINARY PHASE DIAGRAMS[J]. 金属学报, 1996, 32(2): 139-143.
[11] HAO Shiming; ZENG Ninghua (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-16). ISOTHERMAL SECTION OF PHASE DIAGRAM IN Ti-Al-Cr TERNARY SYSTEM AT 1000℃[J]. 金属学报, 1995, 31(16): 152-158.
[12] YAN Licheng;FANG Jianhui;XU Jingyan;YANG Jinxiu(Shanghai University of Science and Technology). PHASE DIAGRAM OF KF-LiCl-CaCl_2 SYSTEM[J]. 金属学报, 1994, 30(19): 301-303.
[13] WAN Jinglong(Anhui Institute of Technology; Hefei); BI Qinghua(Shanghai University of Science and Technology). Gd-CoAl VERTICAL SECTION OF Gd-Co-Al PHASE DIAGRAM[J]. 金属学报, 1994, 30(17): 204-207.
[14] XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2[J]. 金属学报, 1994, 30(16): 150-155.
[15] SHEN Jianyun(General Research Institute for Non-Ferrous Metals;Beijing);CHATILLON C(Laboratoire de Thermodynamique et Physico-chimie Metallurgiques;Fracne)(Manuscript received 16 June;1993). THERMODYNAMICS OF Ga-In-As SYSTEM UNDER LATTICE DEFORMATION[J]. 金属学报, 1994, 30(16): 145-149.
No Suggested Reading articles found!